PTB7-Th (PCE10, PBDTTT-EFT)


Product Code M0261A6-1g
Price $3,600

High Purity, New Generation OPV Donor Polymer

Increased efficiency and more stable than PTB7


Overview | Specifications | MSDS | Literature and Reviews | Technical Support


PTB7-Th, also known as PCE10 or PBDTTT-EFT, is in the new generation of OPV donor polymers that could deliver on the heralded 10/10 target of 10% efficiency and 10 years lifetime. This material has already shown impressive potential with in excess of 9% efficiency reported in the literature and over 7% produced when using large area deposition processes in air with a standard architecture [1,2]. In our own labs we have achieved efficiencies of over 9%.

The advantages of PCE10 are that not only does the material lower HOMO/LUMO levels and increase the efficiencies compared to PTB7 but, more significantly, it is also far more stable. Early indications are that it can be handled under ambient conditions without issues, suggesting that we can look forward to measuring the long term lifetime of the devices.

The Luminosyn™ Range


High Purity Materials: Purified by Soxhlet extraction with methanol, hexane, and chlorobenzene under argon atmosphere.
Batch-Specific Data: Confidence in your materials with batch-specific GPC data for your thesis or publications.
Large Quantity Orders: Plan your experiments with confidence using polymers from the same batch.

General Information


CAS Number 1469791-66-9
Full Name Poly[4,8-bis(5-(2-ethylhexyl)thiophen-2-yl)benzo[1,2-b;4,5-b']dithiophene-2,6-diyl-alt-(4-(2-ethylhexyl)-3-fluorothieno[3,4-b]thiophene-)-2-carboxylate-2-6-diyl]
Chemical Formula (C49H57FO2S6)n
HOMO / LUMO HOMO = 5.24 eV, LUMO = 3.66 eV [1]
Optical λmax = 720 nm; λedge = 785 nm; Eg (optical) = 1.58 eV
Soluble In Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chloroform
Synonyms PCE10, PBDTT-FTTE, PTB7-Th
Classification or Family Thienothiophene, Benzodithiophene, Heterocyclic five-membered ring, Organic semiconducting materials, Low band gap polymers, Organic Photovoltaics, Polymer Solar Cells, All-PSCs, NF-PSCs

Batch Details


Batch Number MW MN PDI Stock Info
M0261A6 135,141 53,926 2.51 In stock

Chemical Structure


PTB7-Th chemical structure
PTB7-Th (PCE10) chemical structure, CAS No. 1469791-66-9

Applications


PCE10 is one of the most exciting materials to have made it out of the labs in recent years and offers huge potential for more in depth research. We'll be working hard over the next few months to maximize efficiencies by optimizing the device architecture, and we will provide further results as we do so. In the mean time, our current fabrication routine is below, and should you have any further questions or queries please contact us.

Ossila's PTB7-Th was used in a high impact paper (IF 18.81)

PTB7-Th from Ossila was used in the high-impact paper (IF 18.81), Copper(I) Thiocyanate (CuSCN) Hole-Transport Layers Processed from Aqueous Precursor Solutions and Their Application in Thin-Film Transistors and Highly Efficient Organic and Organometal Halide Perovskite Solar Cells, N Wijeyasinghe et al., Adv. Funct. Mater., 1701818 (2017); DOI: 10.1002/adfm.201701818.

MSDS Documentation


PTB7-Th MSDSPTB7-Th MSDS sheet

References


  1. Side Chain Selection for Designing Highly Efficient Photovoltaic Polymers with 2D-Conjugated Structure, S. Zhang et al., Macromolecules, 47, 4653-4659 (2014)
  2. Highly Efficient 2D-Conjugated Benzodithiophene-Based Photovoltaic Polymer with Linear Alkylthio Side Chain, L. Ye et al., Chemistry of Materials., 26, 3603-3605 (2014)

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message