TADF Red Dopants
Often coupled with donor-acceptor structures, TADF red dopants are designed for high-efficiency TADF-OLEDs to produce pure red light. Key examples include those based on anthraquinone (AQ) cores like AQ(PhDPA)2 or complex donor-acceptor-donor (D-A-D') systems, featuring units like triphenylamine (TPA) and cyano-functionalized acceptors to achieve small energy gaps (ΔEST) and efficient triplet-to-singlet conversion for near 100% internal quantum efficiency without heavy metals
3DPA-DiKTa is a multiple resonance TADF (MR-TADF) pure red emitter with three electron-donating diphenylamine (DPA) units symmetrically attached to an electron-accepting acridine-5,9-dione (DiKTa) core. Explore our range of high purity TADF red dopant materials for the next generation of OLED devices.