DtBuCzB


Product Code M2493B1-1g
Price $1,050

Blue Dopant Material with Carbazole-based Triphenylboron

High purity sublimed narrowband multi-resonance thermally activated delayed fluorescent (MR-TADF) emitter for highly efficient OLEDs, 2,5,15,18-Tetrakis(1,1-dimethylethyl)-indolo[3,2,1-de]indolo[3',2',1':8,1][1,4]benzazaborino[2,3,4-kl]phenazaborine, BCz-BN, CAS No. 2170487-30-4, Unsublimed ≥97.0%, Sublimed ≥99.0%


DtBuCzB is a carbazole-based triphenylboron MR-TADF material. DtBuCzB has a skeleton structure of CzBN with four bulky peripheral tert-butyl side groups that are evenly distributed on the 3,6-positions of two carbazole rings. The extended π-conjugation generated intensified oscillator strength with narrow greenish blue emission at 481 nm, a FWHM of 22 nm, and a PLQY of 91% in dilute toluene solution. Red-shifted emission spectrum is observed in the corresponding OLED devices producing a high color purity emission at 488 nm, FWHM of 29 nm and maximum EQE of 21.6%.

unsublimed t-DABNA >99.0%, sublimed t-DABNA >99.5%

Sublimed grade

High purity >99.0%

Worldwide shipping

Worldwide shipping

Quick and reliable shipping

Developing longer life-time OLEDs 1802003-07-1

Developing MR-TADF materials

High external quantum efficiency of 21.6%

Narrow band emission 1802003-07-1

Narrow band emission

Full-width half-maximum of 29 nm

DtBuCzB has a similar structure to t-DABNA with the phenyl rings from two two phenylamines being joined to form two side carbazolyl substructures. Due to the extended conjugation by connecting the phenyl rings, DtBuCzB is relatively red-shifted in absorption and emission while compared with those of t-DABNA.

General Information


CAS number 2170487-30-4
Chemical formula C46H49BN2
Molecular weight 640.7 g/mol
Absorption* λmax 467nm (Toluene)
Fluorescence λem 481 nm (Toluene)
HOMO/LUMO HOMO = - 5.30 eV, LUMO = - 2.80 eV
Synonyms 2,5,15,18-Tetrakis(1,1-dimethylethyl)-indolo[3,2,1-de]indolo[3',2',1':8,1][1,4]benzazaborino[2,3,4-kl]phenazaborine, BNCz, BCz-BN
Classification / Family Triphenylboron, Blue dopant, Multiresonance thermally activated delayed fluorescent (MR-TADF), Sublimed materials.

Product Details


Purity Sublimed >99% (HPLC) and unsublimed > 97% (HPLC)
Melting point Tm = 378 °C
Appearance White to yellow powder/crystals

* Sublimation is a technique used to obtain ultra pure-grade chemicals, see sublimed materials for OLED devices.

Chemical Structure


2,6-Bis(3,6-di-tert-butyl-9H-carbazol-9-yl)boron (DtBuCzB) chemical structure, CAS 2170487-30-4

Device Structure(s)


Device structure ITO/TAPC (50 nm)/TCTA (5 nm)/mCBP:1 wt.% DtBuCzB (30nm)/ TmPyPB (30nm)/LiF (1 nm)/Al (100 nm) [1]
Color blue light emitting device Greenish Blue light emission at 488 nm
FWHM 29 nm
CIE coordinates (0.01, 0.42)
Max EQE 21.6%

MSDS Documentation


dtbuczb - 2170487-30-4 - 2,6-bis(3,6-di-tert-butyl-9H-carbazol-9-yl)boronDtBuCzB MSDS Sheet

Literature and Reviews


  1. Y. Xu et al. (2020); Molecular-Structure and Device-Configuration Optimizations toward Highly Efficient Green Electroluminescence with Narrowband Emission and High Color Purity, Adv. Opt. Mater., 8 (9), 1902142; DOI: 10.1002/adom.201902142.
  2. B. Yang et al. (2024); An electrochemically responsive B–O dynamic bond to switch photoluminescence of boron-nitrogen-doped polyaromatics, Nat. Commun., 15, 5166; DOI: 10.1038/s41467-024-48918-6.
  3. S. Tang et al. (2023); Introducing MR-TADF Emitters into Light-Emitting Electrochemical Cells for Narrowband and Efficient Emission, Adv. Funct. Mater., 33 (42), 2306170; DOI: 10.1002/adfm.202306170.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message