It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

P JET (OLED) PEDOT:PSS


Product Code M129-25ml
Price $315

Blue Water-Based pH Neutral PEDOT:PSS Dispersion

Used for applications in HIL and OFET backplanes


Specifications | MSDS | Resources and Support


Production of P JET has been discontinued. Only available while stock lasts. See P JET X N (aqueous) and HIL 8 (organic solvent) for alternatives.

P JET (OLED), CAS number 155090-83-8, is a blue water-based pH neutral PEDOT:PSS dispersion formulated for inkjet printing. As a hole injection layer and antistatic material, P JET (OLED) finds application in OLED and QLED devices to improve the performance and processing of displays, as well as OFET backplanes.

Neutral pH

Neutral pH

Allowing transmission of light to pass into active layer

Versatile P JET (OLED) PEDOT:PSS

Versatile Use

Used for applications in HIL and OFET backplanes

High quality P JET (OLED) PEDOT:PSS

High Quality

Quality formulation

Low conductivity

Tailored Low Conductivity

Low conductivity

Technical Data


Product Name Clevios™ P JET (OLED)
Solvent Water
Composition PEDOT/PSS (1:6 w/w)
CAS Number 155090-83-8
Solid Content 1.6 – 2.1 wt.%
Work Function 5.2 eV approx
Resistivity 1000 – 15000 Ω.cm
Sheet Resistance +10E6 Ω/sq
Conductivity Low conductivity
Particle Size Distribution N/A
Viscosity 4 – 20 mPa.s
pH Value 4.0 – 7.0
Packaging 25 ml of solution sealed in a light resistant bottle with temperature indicator
Storage 3 – 5 °C

Spin Speed Data


P JET (OLD) Spin Speed / Film ThicknessP JET (OLD) Spin Speed / Film Thickness

MSDS Document


P JET (OLD) MSDS SheetP JET (OLED) PEDOT:PSS MSDS Sheet

Related Products


Resources


PEDOT:PSS Deposition How to Spin Coat PEDOT:PSS

For the deposition of thin films of PEDOT:PSS on a freshly prepared surface, we recommend using a vacuum-free spin coater and following this five-step process:

Read more...
PEDOT and PEDOT:PSS Synthesis PEDOT and PEDOT:PSS Synthesis

PEDOT synthesis involves the oxidative chemical or electrochemical polymerization of EDOT monomer. The choice of counterions and polymerization method significantly affects the conductivity, work function, and stability of the resulting PEDOT polymer.

Read more...

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message