It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Highly Conductive Blue PEDOT:PSS Dispersion

Used in transparent electrodes, smart windows, liquid crystal and touch displays, pressure sensors, and wearable electronics


Specifications | MSDS | Resources and Support


F ET PEDOT:PSS (CAS number 155090-83-8) is an aqueous PEDOT:PSS dispersion which is made as a formulation containing polymeric binder resins and functional additives designed for better film quality and processability. Similar to PH 1000 PEDOT:PSS, the ready-to-use F ET PEDOT:PSS ink is one of the most conductive range of PEDOT:PSS products with high Seebeck coefficient and promising thermoelectric (TE) power factors around 30 μW m–1 K–2.

F ET PEDOT:PSS finds application in transparent electrode, conductive textiles, touch displays, pressure sensors. It can be easily deposited either by a range of processes including spin coating, dip-coating, and slot die coating. Studies show that nitrogen gas plasma treatments of F ET PEDOT:PSS coated wool fabrics provide more intense color while retaining its electrical conductivity.

Versatile use

Versatile Use

Wide range of applications

High quality

High Quality

Quality formulation and tailored high conductivity

Enhanced film quanlity

Enhanced Film Quality

Designed with the addition of polymeric binder resins

Worldwide shipping for 1402460-84-7

Worldwide Shipping

Quick and reliable shipping

Technical Data


Product Name Clevios™ F ET
Solvent Water
Composition PEDOT:PSS
Solid Content 3.0 – 4.0 wt.%
Sheet Resistance 100 – 1000 Ω/sq
Conductivity 200 S/cm
Particle Size Distribution N/A
Viscosity 20 – 80 mPa.s at 20°C (100 s-1)
pH Value N/A
Packaging 100 ml of solution sealed in a light resistant bottle with temperature indicator
Storage 3 – 5 °C

Spin Speed Data


F ET Spin Speed / Film ThicknessF ET PEDOT:PSS Spin Speed / Film Thickness

MSDS Document


F ET PEDOT:PSS MSDS MSDS SheetF ET PEDOT:PSS MSDS Sheet

Related Products


Resources


PEDOT:PSS Deposition How to Spin Coat PEDOT:PSS

For the deposition of thin films of PEDOT:PSS on a freshly prepared surface, we recommend using a vacuum-free spin coater and following this five-step process:

Read more...
PEDOT and PEDOT:PSS Synthesis PEDOT and PEDOT:PSS Synthesis

PEDOT synthesis involves the oxidative chemical or electrochemical polymerization of EDOT monomer. The choice of counterions and polymerization method significantly affects the conductivity, work function, and stability of the resulting PEDOT polymer.

Read more...

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message