Titanium Dioxide (TiO2) P25 Nanoparticles
CAS Number 13463-67-7
Cathode Active Materials, Metal Oxides, Anode Active Materials, Advanced Ceramic Materials,Download MSDS
Please choose the appropriate MSDS from the list below. Links will open in a new window. If your browser does not support PDFs, you will be prompted to download the file instead.
Titanium Dioxide (TiO2) P25 Nanopowder
High purity (> 99.5 %) titanium dioxide P25 for applications in DSSCs, photocatalysts and energy storage devices
Technical Data | MSDS | Literature and Reviews | Related Products | Technical Support
Titanium dioxide (TiO2) P25 is widely used as a photocatalyst, particularly in the detoxification of aqueous effluents. Its hydrophilic nature with high specific surface area make it highly effective in photocatalytic applications. Under mild conditions, TiO2 P25 is capable of converting light energy into electrical or chemical energy, making it useful in a range of environmental and energy-related technologies.
High Purity
>99.5% purity
Versatile use
In DSSCs, photocatalysts and energy storage devices
Wide applications fields
are believed to be environmentally friendly
Worldwide shipping
Quick and reliable shipping
P25 titanium dioxide is composed of a mixture of crystal polymorphs, including anatase, rutile, and amorphous phases. This unique combination of crystal polymorphs enhances its photocatalytic efficiency. The anatase phase provides high activity, while the presence of rutile helps facilitate charge separation and electron transfer, reducing recombination rates of photogenerated electron-hole pairs. The synergistic effect of these phases results in superior photocatalytic efficiency compared to single-phase TiO2 materials.
Technical Data
| CAS Number | 13463-67-7 |
|---|---|
| Chemical Formula | TiO2 |
| Molecular Weight | 79.87 g/mol |
| Chemical Name | Titanium Dioxide |
| Synonyms | Titania, Titanium(IV) Oxide |
| Classification / Family | 2D semiconducting materials, nanomaterials, Photocatalyst, DSSCs |
| Color | White powder |
Product Information
| Product Code | M2394C1 |
|---|---|
| Particle Size | 20 nm |
| Form | P25 |
| Appearance | White powder |
| Purity | > 99.5% |
*For larger orders please contact us to discuss prices.
MSDS Documents
Titanium Dioxide P25 Nanoparticles MSDS Sheet
Literatures
-
The Application of Nano-TiO 2 Photo Semiconductors in Agriculture, Y. Wang et al., Nanoscale Res. Lett., 11, 529 (2016); DOI 10.1186/s11671-016-1721-1.
-
Titanium Dioxide: From Engineering to Applications, X. Kang et al., Catalyst, 9, 191 (2019); DOI:10.3390/catal9020191.
-
Electron transport properties analysis of titanium dioxide dye-sensitized solar cells (TiO2-DSSCs) based natural dyes using electrochemical impedance spectroscopy concept: A review, Sol. Energy, 207, 1088-1121 (2020); DOI: 0.1016/j.solener.2020.07.028.