Rutile Titanium Dioxide (TiO2) Nanoparticles
CAS Number 1317-80-2
Cathode Active Materials, Metal Oxides, Anode Active Materials, Advanced Ceramic Materials,Download MSDS
Please choose the appropriate MSDS from the list below. Links will open in a new window. If your browser does not support PDFs, you will be prompted to download the file instead.
Rutile Titanium Dioxide (TiO2) Nanopowder, Average Particle Size of 28 nm
High purity rutile titanium dioxide (>99.5%) for applications in DSSCs, photocatalysts and energy storage devices
Technical Data | MSDS | Literature and Reviews | Related Products | Technical Support
Rutile titanium dioxide is the most prominent and thermally stable polymorph, making it the dominant phase at elevated temperatures. Unlike anatase and brookite, which irreversibly transform into rutile upon heating, rutile titanium dioxide retains its structure under thermal stress. It also possesses a significantly higher dielectric constant than anatase, enhancing its effectiveness in both photocatalytic and electronic applications. While all three polymorphs exhibit photoactive behavior, rutile titanium dioxide’s superior stability and permittivity make it particularly well-suited for use in advanced materials and device technologies.
High Purity
>99.5% purity
Versatile use
In DSSCs, photocatalysts and energy storage devices
Wide applications fields
are believed to be environmentally friendly
Worldwide shipping
Quick and reliable shipping
Our high-purity rutile titanium dioxide nanoparticles offer a combination of excellent structural, optical, and chemical properties, making them highly versatile for a range of advanced applications. The photocatalytic activity of TiO2 nanopowder enables the conversion of light energy into chemical or electrical energy under mild conditions. These nanomaterials are widely recognized as some of the most effective and practical semiconductors available today. They are extensively used in photocatalysis, dye-sensitized solar cells (DSSCs), energy storage systems, and environmental purification technologies such as air and water treatment.
Technical Data
| CAS Number | 1317-80-2 |
|---|---|
| Chemical Formula | TiO2 |
| Molecular Weight | 79.87 g/mol |
| Chemical Name | Titanium Dioxide |
| Synonyms | Titania, Titanium(IV) Oxide |
| Classification / Family | 2D semiconducting materials, nanomaterials, Photocatalyst, DSSCs |
| Color | White powder |
Product Information
| Product Code | M2394B1 |
|---|---|
| Particle Size | 28 nm |
| Form | Rutile |
| Appearance | White powder |
| Purity | > 99.5% |
*For larger orders please contact us to discuss prices.
MSDS Documents
Titanium Dioxide Rutile Nanoparticles MSDS Sheet
Literatures
- The Application of Nano-TiO 2 Photo Semiconductors in Agriculture, Y. Wang et al., Nanoscale Res. Lett., 11, 529 (2016); DOI 10.1186/s11671-016-1721-1
- Titanium Dioxide: From Engineering to Applications, X. Kang et al., Catalyst, 9, 191 (2019); DOI:10.3390/catal9020191
- Electron transport properties analysis of titanium dioxide dye-sensitized solar cells (TiO2-DSSCs) based natural dyes using electrochemical impedance spectroscopy concept: A review, Sol. Energy, 207, 1088-1121 (2020); DOI: 0.1016/j.solener.2020.07.028
Related Products