Formamidinium Iodide (FAI)


Product Code M552-5g
Price $195

Formamidinium iodide, precursor for optimum solar conversion efficiencies

High quality, low price, and available to buy for fast, secure dispatch


Specifications | MSDS | Pricing and Options | Literature and Reviews | Resources and Support


Formamidinium iodide (CAS number 879643-71-7) is an iodide salt of formamidine, the simplest amidine. Formamidinium iodide is often used as a precusor for synthesizing formamidinium lead iodide applied in perovskite solar cells. Formamidinium lead iodide shows a narrower bandgap than the commonly used methylammonium lead iodide (1.48 eV compared to ~1.57 eV), and hence lies closer to that favorable for optimum solar conversion efficiencies. With an approach of FAPbI3 crystallization by the direct intramolecular exchange of dimethylsulfoxide (DMSO) molecules intercalated in PbI2 with formamidinium iodide, device with performance over 20% has been fabricated.

Perovskite precursor material

Perovskite precursor material

for the synthesis of organic-inorganic hybrid perovskite

Worldwide shipping

Worldwide shipping

Quick and reliable shipping

electronic applications

Used in multiple electronic applications

including FETs, LEDs, and PVs

High purity

High purity

> 99.9% non-recrystallized and recrystallized grade available

Formamidinium Iodide (FAI) from Ossila was used in a high-impact paper (IF 9.229)

Formamidinium Iodide (FAI) from Ossila was used in the high-impact paper (IF 9.229), Using Soft Polymer Template Engineering of Mesoporous TiO2 Scaffolds to Increase Perovskite Grain Size and Solar Cell Efficiency, Q. Lian et al., ACS Appl. Mater. Interfaces 12, 18578–18589 (2020); DOI: 10.1021/acsami.0c02248.

Specifications


CAS number 879643-71-7
Chemical formula CH5IN2
Molecular weight 171.97 g/mol
Synonyms FAI, Formamidine hydroiodide
Classification / Family Perovskite precursor materials, Perovskite solar cells, OLEDs

Product Details


Purity

M552: 99.995% (ICP-OES)

M551: >99.995% (further purified by double recrystallization from 99.9% grade in ethanol)

Melting point 242 °C
Color White powder/crystals

Chemical Structure


Chemical structure of formamidinium iodide
Chemical structure of formamidinium iodide (FAI), CAS No. 879643-71-7
Device structure FTO/TiO2/FAPbIBr2/spiro-OMeTAD/Au [1]
JSC (mA cm-2) 23.3
VOC (V) 0.94
FF (%) 65
PCE (%) 14.2
Device structure FTO/TiO2/(FAPbI3)0.85(MAPbBr3)0.15/PTAA/Au [4]
JSC (mA cm-2) 22.5
VOC (V) 1.11
FF (%) 73.2
PCE (%) 18.4
Device structure FTO/bl-TiO2/mp-TiO2/FAPbI3 (DMSO)/PTAA/Au [5]
JSC (mA cm-2) 24.7
VOC (V) 1.06
FF (%) 77.5
PCE (%) 20.2

Pricing


Grade Order Code Quantity Price
99.995% purity M552 5 g £130
99.995% purity M552 10 g £220
99.995% purity M552 25 g £300
>99.995% purity M551 5 g £200
>99.995% purity M551 10 g £330

MSDS Documentation


Formamidinium Iodide MSDSFormamidinium iodide MSDS sheet

Applications


Formamidinium lead iodide shows a narrower bandgap than the commonly used methylammonium lead iodide (1.48 eV compared to ~1.57 eV), and hence lies closer to that favorable for optimum solar conversion efficiencies [1]. Spin-coating the formamidinium iodide (FAI) plus PbI2 precursor solution in N,N-dimethylformamide (DMF) initially resulted in discontinuous perovskite films. However, by adding a small amount of hydroiodic acid (HI) to the stoichiometric FAI, extremely uniform and continuous films were formed.

Controlled humidity is another deciding factor that affects the film morphology, crystallinity, and optical and electrical properties of FAPbI3 [2]. 16.6% PCE was achieved with low relative humidity of 2%, with the device efficiency dropped to about half (8.6%) when the humidity was 40%.

Low-volatility additives such as FACl and MACl are good candidates for assisting in the crystallization of phase pure α-FAPbI3 via the formation of intermediate mixtures, which prohibits the crystallization of the δ-FAPbI3 phase [3]. It also has been observed that the black perovskite-type polymorph (α-phase), which is stable at relatively high temperatures (above 160 oC), turned into the yellow FAPbI3 polymorph (δ-phase) in an ambient humid atmosphere. Results show that incorporation of MAPbBr3 into FAPbI3 stabilizes the perovskite phase of FAPbI3 and improves the power conversion efficiency of the solar cell to more than 18% under a standard illumination of 100 mW/cm2 [4].

With an approach of FAPbI3 crystallization by the direct intramolecular exchange of dimethylsulfoxide (DMSO) molecules intercalated in PbI2 with formamidinium iodide, device with performance over 20% has been fabricated [5].

Literature and Reviews


  1. Formamidinium lead trihalide: a broadly tunable perovskite for efficient planar heterojunction solar cells, G. E. Eperon et al., Energy Environ. Sci., 7, 982-988 (2014), DOI: 10.1039/C3EE43822H.
  2. Controlled Humidity Study on the Formation of Higher Efficiency Formamidinium Lead Triiodide-Based Solar Cells, S. Wozny et al., Chem. Mater., 27 (13), 4814–4820 (2015), DOI: 10.1021/acs.chemmater.5b01691.
  3. Additive-Modulated Evolution of HC(NH2)2PbI3 Black Polymorph for Mesoscopic Perovskite Solar Cells, Z. Wang et al., Chem. Mater., 27 (20), 7149–7155 (2015), DOI: 10.1021/acs.chemmater.5b03169.

Resources and Support


How to Make Efficient Perovskite Solar Cells in a Glove Box

Various other perovksites and transport materials, along with references and examples of their uses, can be found on our "Ultimate Guide to Perovskites" page - but we thought it would be useful to demonstrate an example of how to make a PSC (that can acheive over 19% PCE), from start to finish. We've also tried to include some helpful tips to perfect your technique.

Learn more...

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message