EPDM MEA and GDE Gasket


Product Code C2058E05
Price $75

EPDM Gasket for MEA Electrolyzers and GDE Flow Cells

Airtight, alkali resistant sealing while securing electrode materials


Specifications | Gallery | Literature | Related Products | Technical Support


EPDM (ethylene propylene diene monomer) is a synthetic copolymer of ethylene, propylene, and ethylidene norbornene. With high tensile strength and elasticity, our EPDM gaskets provide great electrical insulation and are highly resistant to aging, water, steam, weather, ultraviolet radiation, and ozone. With a low compression set, our EPDM gaskets remain highly flexible at temperatures ranging from -45°C to 150°C. 

Ideal for MEA electrolyzers and GDE flow cells, our EPDM gaskets act as a seal to prevent reactant gas and electrolyte leaking, control mechanical compression across the active area, and secure fragile ion exchange membranes in position protecting them from stress and damage during assembly processes and electrochemical reactions.

EPDM exhibits excellent resistance to alkalis such as sodium hydroxide and potassium hydroxide. At normal temperatures it handles dilute and moderately concentrated alkaline solutions well, making it ideal for water treatment, chemical processing, and electrochemical cell settings. EPDM gaskets are preferred to other commonly used materials (PTFE and FKM) to handle alkaline conditions in MEA electrolyzers and GDE flow cells.

Specifications


Material EPDM
Ideal Operating Temperatures -45 - 150°C
Overall Dimensions 52 mm x 52 mm
Available Window Dimensions 12 mm x 12 mm, 23 mm x 23 mm
Available Thicknesses 0.5 mm, 1.0 mm, 1.5 mm, 2.0 mm, 3.0 mm
Pack Size 5
PTFE Gasket Dimension Diagram
EPDM Gasket Dimensions

Literature and Reviews


  1. J. Yoo et al. (2023), Study on low temperature and durability characteristics of gasket for polymer electrolyte membrane fuel cell (PEMFC) depending on cross-sectional geometry, Int. J. Hydrogen. Energy, 50, Part C, 1194-1206; DOI: 10.1016/j.ijhydene.2023.10.145.
  2. Z. Li et al. (2026), Architecting hierarchical networks in EPDM rubber for high-durability sealing of proton exchange membrane electrolysis cells, Int. J. Hydrogen. Energy, 218, 154046; DOI: 10.1016/j.ijhydene.2026.154046.
  3. R. Barros et al. (2025), Impact of nickel electrode geometry on the electrochemical performance and bubble dynamics of a zero-gap alkaline electrolyzer, J. Power. Sources, 630, 236116; DOI: 10.1016/j.jpowsour.2024.236116.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message