High-purity copper foil substrate for use as current collectors in Li-ion anodes and other energy storage applications. This battery grade foil is available in a variety of thicknesses and both single and double sided polish finishes. This gives flexibility in cell design, balancing conductivity and energy density.

Pre-packaged sheets simplify testing different specifications while eliminating the need to store bulky rolls and fit on smaller benchtop bar-coating machines - ready to use straight out of the bag.

In addition to copper foils, we offer a range of anode active materials that can be purchased separately. These materials, such as carbon black and graphite powders, are ideal for coating the foils, enabling the production of highly efficient and stable electrodes tailored to your specific needs.

General Specifications


Dimensions

148 x 210 mm (S2011#1 / S2012#1)

210 x 297 mm (S2011#2 / S2012#2)

Purity

Cu >99.9%

Fe <0.0010%

Bi <0.00020%

Pb <0.0005%

Single Sided Polish

Thickness (µm) 9 12 15
Tensile Strength (MPa) ≥296 ≥305 ≥330
Surface Dyne (dyne/cm) 64 68 70
Normal Elongation (%) 2.6 3.0 3.3
Product Code S2011A1/A2 S2011B1/B2 S2011C1/C2

Double Sided Polish

Thickness (µm) 6 9 12
Tensile Strength (MPa) ≥270 ≥296 ≥305
Surface Dyne (dyne/cm) 61 64 68
Normal Elongation (%) 2.2 2.6 3.0
Product Code S2012A1/A2 S2012B1/B2 S2012C1/C2



Browse our range of anode active materials

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message