It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

4-Pentylphenyl 4-pentylbenzoate


Product Code M2366A1-25g
Price $345

4-Pentylphenyl 4-pentylbenzoate, liquid crystal (nematic)

Liquid crystal for the application of optical electronics i.e. in liquid-crystal display (LCD).


Specifications | Pricing and Options | MSDS | Literature and Reviews


4-Pentylphenyl 4-pentylbenzoate (5PEP5), CAS number 74305-48-9, is a nematic liquid crystal with a chemical structure of 4-pentylphenyl ester of 4-pentylbenzoate.

4-Pentylphenyl 4-pentylbenzoate has a ester link and a core which is more flexible and less directed along the long molecular axis that the biphenyl liquid crystals, i.e. 4'-Heptyl-[1,1'-biphenyl]-4-carbonitrile. However, the observed alignment properties of 4-pentylphenyl 4-pentylbenzoate having two pentyl tails on its self are similar to those of the rode-like biphenyl core molecule 4-pentyl-4’-cyanobiphenyl. The alignment on the substrate polyvinyl imidazole (PVI) is perpendicular to the rubbing direction, perpendicular to the vinyl backbone

Nematic liquid crystal

Nematic liquid crystal

With phenylbenzoate core

Rod-like mesogen

Rod-like mesogen

With two pentyl alkyl chain

Worldwide shipping for 74305-48-9

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>98% High purity

Chemical Structure


chemical structure of 4-Pentylphenyl 4-pentylbenzoate, CAS 74305-48-9
Chemical structure of 4-Pentylphenyl 4-pentylbenzoat, CAS 74305-48-9

General Information


CAS Number 74305-48-9
Chemical Formula C23H30O2
Molecular Weight 338.48
Full Name 4-Pentylphenyl 4-pentybenzoate
Synonyms 5PEP5, Pentylphenyl pentylbenzoate, 4-Amylphenyl 4′propybenzoate, 4-Pentybenzoic acid 4-pentylphenyl ester
Classification / Family Phenyl Ester Liquid Crystals, Nematic Liquid Crystals

Product Details


Purity >97% (1HNMR)
Form White powder/crystals
Melting Point 34.0 - 38.0 °C
Solubility Methanol

Pricing


Batch Quantity Price
M2366A 10 g £115
M2366A 25 g £230
M2366A 50 g £350
M2366A 100 g £520

MSDS Documentation


4-Pentylphenyl 4-pentylbenzoate MSDS4-Pentylphenyl 4-pentylbenzoat MSDS Sheet

Literature and Reviews


  1. Rod-like cyanophenyl probe molecules nanoconfined to oxide particles: Density of adsorbed surface species, S. Frunza et al., Eur. Phys. J. Plus 131, 27 (2016); DOI: 10.1140/epjp/i2016-16027-5
  2. Peculiar orientation of nematic liquid crystals on rubbed polyvinylimidazole, S. Frunza et al., J. Optoelectron. Adv. Mater., 7 (4), 2149-2157 (2005).

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message