4-(trans-4-Pentylcyclohexyl)benzonitrile


Product Code M2358A1-25g
Price $465

4-(trans-4-Pentylcyclohexyl)benzonitrile (PCH5), liquid crystal (nematic).

Nematic liquid crystal for the application of optical electronics i.e. in liquid-crystal display (LCD)


Specifications | Pricing and Options | MSDS | Literature and Reviews


4-(trans-4-Pentylcyclohexyl)benzonitrile (PCH5), CAS number 61204-01-1, has a structure of pentyl alkyl chain and benzonitrile groups attached to 1,4-positions of cyclohexane ring in trans-geometry, in another word, they are facing opposite directions.

4-(trans-4-Pentylcyclohexyl)benzonitrile is a rod-like liquid crystal with a nematic to isotropic phase transition at 327.6 K and a crystalline to nematic phase transition at 303 K. Nematic is one of the liquid crystal phases that molecules that have no positional order however tend to point in the same direction (along the director). The positional order of nematic liquid crystal can be cultivated by physical gelation mainly induced by the formation of intermolecular hydrogen bonds of gelling agents in solvents.

Nematic Liquid crystal

Nematic Liquid crystal

With diastereomer core

Multiple applications

Multiple applications

In optoelectronic and liquid crystal display

Worldwide shipping for 61204-01-01

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>98% High purity

Chemical Structure

4-(trans-4-Pentylcyclohexyl)benzonitrile, CAS 61204-01-1
Chemical structure of 4-(trans-4-pentylcyclohexyl)benzonitrile, CAS 61204-01-1

General Information


CAS Number 61204-01-1
Chemical Formula C18H25N
Molecular Weight 255.40
Full Name 4-(trans-4-Pentylcyclohexyl)benzonitrile
Synonyms PCH5, PCH-5, 5PCH, 1-(trans-4-Amylcyclohexyl)-4-cyanobenzene, 4-(4-Pentylcyclohexyl)benzonitrile
Solubility Methanol
Classification / Family Benzonitrile, Nematic Liquid Crystals

Product Details


Purity >98% (1HNMR)
Form White powder/crystals
Melting Point Tm = 30.0 °C

Pricing


Batch Quantity Price
M2358A1 10 g £155
M2358A1 25 g £310
M2358A1 50 g £500

MSDS Documentation


4-(trans-4-Pentylcyclohexyl)benzonitrile MSDS4-(trans-4-Pentylcyclohexyl)benzonitrile MSDS Sheet

Literature and Reviews


  1. Physical Gelation of Nematic Liquid Crystals with Amino Acid Derivatives Leading to the Formation of Soft Solids Responsive to Electric Field, N. Mizoshita et al., J. Photopolym. Sci. Technol., 13 (2), 307-312 (2000); DOI: 10.2494/photopolymer.13.307.
  2. Molecular Dynamics in the Rod-like Liquid Crystal 4-(trans-4-Pentylcyclohexyl)benzonitrile (PCH5) Probed by Muon Spin Resonance Spectroscopy, I. McKenzie et al., Phys. Procedia 30, 91–96 (2012); DOI: 10.1016/j.phpro.2012.04.047.
  3. Investigation of dielectric, optical and zeta potential properties of pure and zinc ferrite nanoparticles dispersed nematic liquid crystal PCH5. D. Gaur et al., Appl. Phys. A, 128, 230 (2022); DOI: 10.1007/s00339-022-05318-1.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message