It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

PBDB-T (PCE12)


Product Code M1001A4-1g
Price $2,550

High Performing Polymer Donor for OPVs

Reported efficiencies exceeding 12% and a certified efficiency approaching 11%


Specifications | MSDS | Literature and Reviews | Technical Support


PBDB-T (also known as PCE12) is one of the highest performing donor polymers for OPVs, having reported efficiencies exceeding 12% and a certified efficiency approaching 11%. These efficiencies were achieved when PBDB-T was used in conjunction with recently-reported non-fullerene acceptors (NFAs, including ITIC) in inverted architecture devices. These devices also exhibited excellent thermal stability, making the combination a promising candidate for the proposed 10/10 target of 10% efficiency and 10-year lifetimes.

PBDB-T (PCE12) from Ossila was used in a high-impact paper

PBDB-T (PCE12) from Ossila was used in the high-impact paper (IF 29.37), Sequentially Deposited versus Conventional Nonfullerene Organic Solar Cells: Interfacial Trap States, Vertical Stratification, and Exciton Dissociation, J. Zhang et al., Adv. Energy Mater., 1902145 (2019); DOI: 10.1002/aenm.201902145; and paper (IF 29.37), Design Rules for Polymer Blends with High Thermoelectric Performance, O. Zapata-Arteaga et al., Adv. Energy Mater., 12, 2104076 (2022); DOI: 10.1002/aenm.202104076.

PBTB-T (PCE12) is easy to process, simplifying device fabrication (using a glove box) while simultaneously providing high performance. Due to good HOMO alignment with the valence band of commonly-used perovskites, this polymer could also be potentially used as a hole-transporting material in perovskite solar cells.

Contact us for large orders over 1 gram with a lead time of 4-6 weeks.

The Luminosyn™ Range


High Purity Materials: Purified by Soxhlet extraction with methanol, hexane, and chlorobenzene under argon atmosphere.
Batch-Specific Data: Confidence in your materials with batch-specific GPC data for your thesis or publications.
Large Quantity Orders: Plan your experiments with confidence using polymers from the same batch.

General Information


Full Name Poly[(2,6-(4,8-bis(5-(2-ethylhexyl)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene))-alt-(5,5-(1’,3’-di-2-thienyl-5’,7’-bis(2-ethylhexyl)benzo[1’,2’-c:4’,5’-c’]dithiophene-4,8-dione))]
Synonyms PBDB-T, PBDTBDD
Chemical Formula (C68H78O2S8)n
CAS Number 1415929-80-4
HOMO / LUMO HOMO = -5.33 eV, LUMO = -2.92 eV [3]
Solubility Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chlorobenzene - M1001A3, Dichlorobenzene or Chlorobenzene+dichlorobenzene (1:1 v/v) - M1001A4
Classification or Family

Organic semiconducting materials, Medium band-gap polymers, Organic Photovoltaics, Polymer solar cells, Perovskite solar cells, Hole-transport layer materials, NF-PSCs, All-polymer solar cells (all-pscs).

Batch Details


Batch number MW Mn PDI Stock info
M1001A4 115,662 49,146 2.35 In stock

Chemical Structure


Chemical structure of PBDB-T (PCE12)
Chemical structure and product image of PBDB-T (PCE12)

Device Structure(s)


The device structure of the certified devices was ITO / ZnO (30 nm) / PBDB-T:ITIC (100 nm) / MoO3 (10 nm) / Al (100 nm), with PBDB-T:ITIC solution details as follows:

  • Blend ratio: 1:1,
  • Concentration: 20 mg/ml,
  • Solvent: Chlorobenzene
  • Additive: 0.5% Diiodooctane.

MSDS Documentation


PBDB-T MSDSPBDB-T MSDS sheet

Literature and Reviews


  1. Energy-Level Modulation of Small-Molecule Electron Acceptors to Achieve over 12% Efficiency in Polymer Solar Cells, S. Li et al, Adv. Mater., 28, 9423–9429 (2016); DOI: 10.1002/adma.201602776.
  2. Ternary Polymer Solar Cells based on Two Acceptors and One Donor for Achieving 12.2% Efficiency, W. Zhao et al., Adv. Mater., 29, 1604059 (2017); DOI: 10.1002/adma.201604059.
  3. Fullerene-Free Polymer Solar Cells with over 11% Efficiency and Excellent Thermal Stability, W. Zhao et al., Adv. Mater., 28, 4734–4739 (2016); DOI: 10.1002/adma.201600281.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message