It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

Lithium Aluminum Titanium Phosphate (LATP) Powder

CAS Number 120479-61-0

Battery Materials, Materials

Product Code M2556A1-25g
Price $210

A Lithium Analog of NASICON

Promoting high ionic conductivity in solid-state lithium-ion batteries


Product Information | MSDS | Literature & Reviews | Related Products


Lithium aluminum titanium phosphate (LATP, CAS number: 120479-61-0) is a lithium analog of the sodium super ionic conductor (NASICON) commonly used as a solid-state electrolyte for all-solid-state batteries. LATP is considered an aluminum-doped lithium titanium phosphate (LTP) showing an ionic conductivity 3 to 4 orders of magnitude higher than that of LTP. Being a NASICON-type electrolyte, lithium aluminum titanium phosphate exhibits high ionic conductivity in the range of 10−4 to 10−3 S/cm. LATP also has good chemical stability and high oxidation voltage (ca. 6 V).

LATP can be further functionalized by a coupling agent (such as silanes) to enhance its interaction with polymers for quasi-solid-state electrolytes, achieving an ionic conductivity of 3.01 × 10−3 S/cm.

High Ionic Conductivity

In the range of
10−4 to 10−3 S/cm

Low Cost Material

For affordable and effective battery R&D

Highly Stable Electrolyte

For safe solid-state
batteries

Worldwide Shipping

Reliable delivery via tracked courier as standard

General Information


CAS Number 120479-61-0
Chemical Formula Li1.3Al0.3Ti1.7(PO4)3
Full Name Lithium aluminum titanium phosphate
Molecular Weight 383.41 g/mol
Synonyms LATP, Al-doped lithium titanium phosphate
Classification or Family NASICON-type electrolyte, Solid state electrolyte, Battery materials, ASSBs

Product Details


Particle Size 0.639 μm (D50)
Specific Surface Area 14.47 m2/g
Ionic Conductivity 6.69 × 10−4 S/cm at 25°C (EIS)
Appearance White powder

MSDS Documentation


Lithium Aluminum Titanium Phosphate (LATP) Powder MSDS SheetLithium Aluminum Titanium Phosphate (LATP) Powder MSDS Sheet

References


  • Recent advances in conduction mechanisms, synthesis methods, and improvement strategies for Li1+xAlxTi2-x(PO4)3 solid electrolyte for all-solid-state lithium batteriesP. Wu et al., Adv. Energy Mater., 13, 2203440 (2023); DOI: 10.1002/aenm.202203440.
  • Amine-functionalized silane-modified LATP nanofillers in PVDF-HFP: a quasi-solid-state electrolyte for Li-ion batteries, P. Bharathi et al., ACS Appl. Nano Mater., 8, 16706–16716 (2025); DOI: 10.1021/acsanm.5c02618.
  • Understanding the positive effect of LATP in polymer electrolytes in all-solid-state lithium batteries, O. Breuer et al., J. Electrochem. Soc., 170, 090509 (2023); DOI: 10.1149/1945-7111/acf482.


We stock a wide range of Battery materials available to purchase online. Please contact us if you cannot find what you are looking for.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message