ITIC-Th, IT-Th

CAS Number 1889344-13-1

Non-Fullerene Acceptors, Materials

Product Code M2074A1-500mg
Price $1,635

ITIC-Th, non-fullerene acceptor with deep energy levels

Low price, high purity (≥99%) ITIC-Th with free shipping on qualifying orders


Specifications | Pricing and Options | MSDS | Literature and Reviews


ITIC-Th (CAS number 1889344-13-1), also known as IT-Th, is an ITIC derivative and a non-fullerene acceptor. Compared with ITIC, instead of having phenyl side-chains, ITIC-Th has hexylthienyl side chains which promotes intermolecular interaction and, therefore, the electron mobility induced by sulfur–sulfur interaction.

High efficient non-flullerene acceptor

High efficient non-fullerene acceptor

with highly conjugated core

Improve electron mobility

Improve electron mobility

Induced by sulfur-sulfur interaction

Worldwide shipping for 1889344-13-1

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>99% High purity

ITIC-Th from Ossila was used in the high-impact paper (IF 18.81)

ITIC-Th from Ossila was used in the high-impact paper (IF 18.81), Polymorphism in Non-Fullerene Acceptors Based on Indacenodithienothiophene, S. Marina et al., Adv. Funct. Mater., 2103784 (2021); DOI: 10.1002/adfm.202103784.

ITIC-Th also shows lower energy levels (HOMO = −5.66 eV, LUMO = −3.93 eV) than ITIC due to the effect of thienyl side-chains. With even deeper energy levels, it can potentially match the energy levels of most of the high-performance narrow, medium, to wide band-gap polymer semiconductor donors.

Chemical Structure

Chemical structure of ITIC-Th
Chemical structure of ITIC-Th, CAS number: 1889344-13-1

General Information


CAS Number 1889344-13-1
Chemical Formula C86H74N4O2S8
Purity >99% (1H NMR)
Full Name 3,9-bis(2-methylene-(3-(1,1-dicyanomethylene)-indanone))-5,5,11,11-tetrakis(5-hexylthienyl)-dithieno[2,3-d:2’,3’-d’]-s-indaceno[1,2-b:5,6-b’]dithiophene
Molecular Weight 1452.05 g/mol
HOMO / LUMO HOMO = -5.66 eV, LUMO = -3.93 eV [1]
Solubility Chloroform, chlorobenzene, dichlorobenzene
Synonyms IT-Th
Classification / Family NFAs, organic semiconducting materials, low band-gap small molecule, small molecular acceptor, organic photovoltaics, polymer solar cells, NF-PSCs, n-type acceptor

Pricing


Batch Quantity Price
M2074A1 100 mg £320
M2074A1 250 mg £640
M2074A1 500 mg £1090

MSDS Documentation


ITIC-Th MSDSITIC-Th MSDS Sheet

Literature and Reviews


  1. High-Performance Electron Acceptor with Thienyl Side Chains for Organic Photovoltaics, Y. Lin et al., J. Am. Chem. Soc., 138 (14), 4955–4961 (2016); DOI: 10.1021/jacs.6b02004.
  2. Ternary Organic Solar Cells Based on Two Compatible Nonfullerene Acceptors with Power Conversion Efficiency >10%, Adv. Mater., 28, 10008–10015 (2016); DOI: 10.1002/adma.201602570.
  3. Side-Chain Isomerization on an n‑type Organic Semiconductor ITIC Acceptor Makes 11.77% High Efficiency Polymer Solar Cells, Y. Yang et al., J. Am. Chem. Soc., 138, 15011−15018 (2016); DOI: 10.1021/jacs.6b09110.

Related Products


Non-Fullerene Acceptors Collection

Non-Fullerene Acceptors

Non-Fullerene Acceptors

Non-fullerene acceptors (NFAs) are a promising alternative to fullerene-based electron acceptors.

Semiconducting Polymers Collection

Semiconducting Polymers

Semiconducting Polymers

Semiconducting polymers for bulk heterojunction, OPV, OLED, OFET and perovskite interfaces and solar cell research.

Organic Conductors Collection

Organic Conductors

Organic Conductors

Organic conductors are an environmentally friendly alternative to traditional inorganic conductors.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message