It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

FTO Glass Substrates, 25 mm Square, PV and OLED


Product Code S2008C1-100
Price $600

Patterned FTO Substrates for Rapid OLED and PV Prototyping

Large pixels for record breaking-devices


Specifications | Related Products | Resources and Support


The 25 mm square substrates have been designed to help the community take the next step in scaling up active areas. When combined with our deposition masks, these substrates allow four pixels per substrate, with active areas of 48 mm2 each, or a single large pixel with an active area of 255 mm2 .

Specifications


Substrate size 25 mm x 25 mm
Thickness 1.6 mm
Glass type Polished soda lime, float glass
Substrate coating FTO
FTO thickness 300 nm
FTO resistance 6 - 9 Ω/square
Pixel Sizes 48 mm2 (6 mm x 8 mm) or 255 mm2 (15 mm x 17 mm)
ITO 25 x 25 substrate schematic

Resources and Support


OLED Fabrication GuideOLED Fabrication Guide

Fabricating OLED devices using Ossila’s pre-patterned substrates is designed to be quick and easy. We've included every detail that we can in this manual so that you can produce efficient devices with as little effort as possible.

Read more...
OPV Fabrication GuideOPV Fabrication Guide

Within this guide, you’ll find comprehensive explanations for each step, along with additional tips and insights we’ve gathered to help you achieve the best possible results.

Read more...