It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

bis-PCBM (PC60BM Bisadduct)


Product Code M191-500mg
Price $1,140

Improve Open Circuit Voltage of Solar Cells

For OPV applications and crystallization studies


Product Information | MSDS | Literature and Reviews | Resources and Support


Bis(1-[3-(methoxycarbonyl)propyl]-1-phenyl)-[6,6]C62 or bis[C60]PCBM, also known as a PCBM bisadduct, is used to increase the open circuit voltage of solar cells by approximately 0.1 V due to the higher lying LUMO level [1]. This material is also used in crystallization studies, especially when comparing polymer-fullerene packing [2,3].

High purity 1048679-01-1

High Purity

>99.5% material purity

Soluble fullerene acceptor

Soluble Fullerene Acceptor

For high efficiency OPVs

Higher lying LUMO energy level

Higher Lying LUMO Energy Level

Improve open circuit voltage

Worldwide shipping for 1048679-01-1

Worldwide Shipping

Quick and reliable shipping

Product Information


CAS number 1048679-01-1
Purity >99.5%
Molecular Weight 1101.1 g/mol

Chemical Structure


bis-PCBM chemical structure
bis-PCBM (PC60BM Bisadduct), CAS 1048679-01-1

Pricing


Product Code Purity Quantity Price
M191 >99.5% 200 mg £380
M191 >99.5% 500 mg £760

MSDS Documentation


bis-PCBM MSDSbis-PCBM MSDS Sheet

Literature and Reviews


  1. Fullerene Bisadducts for Enhanced Open-Circuit Voltages and Efficiencies in Polymer Solar Cells, M. Lenes et al., Advanced Materials, 20, 2116 (2008)
  2. Tuning the Properties of Polymer Bulk Heterojunction Solar Cells by Adjusting Fullerene Size to Control Intercalation, N. Cates et al., Nano Letters, 9, 4153 (2009)
  3. Effects of Intercalation on the Hole Mobility of Amorphous Semiconducting Polymer Blends, N. Cates et al., Chemistry of Materials, 22, 3543 (2010)

Resources and Support


Polymer-Fullerene Bulk Heterojunction Solar Cells Polymer-Fullerene Bulk Heterojunction Solar Cells

Polymer-fullerene bulk heterojunction (BHJ) solar cells are based on blends of semiconducting polymers and fullerene derivatives, such as PCBM. It is described as a bulk heterojunction as it involves a blend of two materials with differing energy band gaps, forming a dispersed, interpenetrating network.

Read more...

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message