Covalent Organic Frameworks (COFs) Terephthalaldehyde Ligand

A dialdehyde ligand for the synthesis of COFs and semiconductors in applications of OLEDs, solar cells, and memristors.


Overview | Product Information | Related Products


2,5-Bis(octyloxy)terephthalaldehyde (CAS number 123440-34-6) is a benzene building block with two aldehydes and two n-octyloxy groups. 2,5-Bis(octyloxy)terephthalaldehyde is commonly used for synthesizing covalent organic frameworks (COFs) with amine derivatives such as triaminophenylbenzene. Through the imination reaction of amine and aldehyde, the resulting COF exhibits BET surface area of 1202 m2/g. These porous COFs are applied in memristors with an on/off ratio of an order of magnitude.

In addition to COFs, 2,5-bis(octyloxy)terephthalaldehyde is a synthesis intermediate for vinylene-bridged macromolecules. Such macromolecules have extended π-conjugation, enhancing the charge carrier mobility of organic semiconductors. The fully conjugated backbone allows the resulting polyimine to be used in photovoltaic with power conversion efficiency of 0.17% (preliminary study).

MOF and COF ligands

MOF and COF ligands

Aldehyde ligand for cross-linked COF/MOF networks

Facile reactions

Facile reactions

Aldehyde possesses excellent reactivity

High purity

High purity

> 98% pure

Worldwide shipping

Quick and reliable shipping

General Information

CAS Number 123440-34-6
Chemical Formula C24H38O4
Full Name 2,5-Bis(octyloxy)terephthalaldehyde
Molecular Weight 390.56 g/mol
Synonyms 2,5-dioctyloxybenzene-1,4-dicarbaldehyde, C8PDA
Classification or Family Carbaldehyde monomers, Alkylated monomers, COFs, Porous organic frameworks

Chemical Structure


2,5-Bis(octyloxy)terephthalaldehyde chemical structure, CAS 123440-34-6
2,5-Bis(octyloxy)terephthalaldehyde chemical structure, CAS 123440-34-6

Product Details

Purity > 98%
Melting Point 76 – 79 °C
Appearance Bright yellow powder

MSDS Documentation

2,5-Bis(octyloxy)terephthalaldehyde MSDS Sheet2,5-Bis(octyloxy)terephthalaldehyde MSDS Sheet

References

  • Effect of functional groups on microporous polymer based resistance switching memory devices, Y. Song et al., Chem. Commun., 56, 6356–6359 (2020); DOI: 10.1039/D0CC01397H
  • Novel vinylene-bridged donor–acceptor copolymers: synthesis, characterization, properties and effect of cyano substitution, C. Wei et al., Mater. Chem. Front., 1, 2103 (2017); DOI: 10.1039/c7qm00236j.
  • Understanding degradation dynamics of azomethine-containing conjugated polymers, A. Charland-Martin et al., Macromolecules, 57, 6145–6155 (2024); DOI: 10.1021/acs.macromol.4c01168.

We stock a wide range of Porous Organic Frameworks available to purchase online. Please contact us if you cannot find what you are looking for.