Single Crystal NMC631 Powder
CAS Number 346417-97-8
Lithium Nickel Manganese Cobalt Oxide, Cathode Interlayer Materials (CIMs), Cathode Active Materials, Metal Oxides,Enhanced Thermal Stability and Extended Cycle Life
Optimized mid-nickel cathode for high-performance lithium-ion batteries
Specifications | MSDS | Literature | Related Products | Technical Support
Single crystal NMC631 (CAS 346417-97-8) is a mid-nickel cathode material engineered to deliver an optimal balance of energy density, thermal stability, and long-term durability. Compared to high-nickel NMC materials, this powder offers enhanced thermal stability and extended cycle life. Additionally, it provides higher energy density than low-nickel NMC compositions, making it an ideal "performance-stability balance" material. Unlike conventional polycrystalline cathodes that form secondary agglomerated particles, single crystal NMC631 consists of discrete, robust primary particles. The absence of internal grain boundaries significantly reduces microcracking during cycling.
This material also demonstrates excellent thermal compatibility with solid-state electrolytes such as LLZTO, maintaining structural phase integrity at temperatures up to 1000 °C. In all-solid-state lithium batteries (ASSLBs), single crystal NMC631 powder exhibits reduced capacity loss of 48%, attributed to improved interfacial stability.
High Specific Energy Density
Promising future cathode material
Low Cost
Affordable battery R&D
Versatile Material
EVs, power tools, and energy storage
Worldwide Shipping
Quick and reliable shipping
General Information
| CAS Number | 346417-97-8 |
|---|---|
| Chemical Formula | LiNi0.6Mn0.3Co0.1O2 |
| Full Name | Lithium nickel manganese cobalt oxide |
| Molecular Weight | 96.52 g/mol |
| Synonyms | Single crystal NMC631, Single crystal NCM631, NMC631 single crystal powder, SC NMC631, Cobalt lithium manganese nickel oxide |
| Classification or Family | Battery materials, Metal oxides, Cathode materials, Advance ceramic materials |
Morphology
Product Details
| Tab Density | 1.5 g/cm3 |
|---|---|
| Specific Surface Area | 0.84 m2/g |
| Particle Size | 4.29 µm (D50) |
| First Discharge Capacity (0.5C) | ≥ 182.6 mAh/g |
| First Columbic Efficiency | ≥ 88% |
| Appearance | Dark gray powder |
MSDS Documentation
Single crystal NMC631 powder MSDS Sheet
Literature
- Thermal stability and electrochemical behavior of commercial polycrystalline and single-crystalline cathodes integrated with cubic Li6.4La3Zr1.4Ta0.60O12 for all-solid-state lithium batteries, Z. Ma et al., J. Mater. Chem. A, 13, 26647–26659 (2025); DOI: 10.1039/D5TA03114A.
- Designing surface coating strategies with tungsten on single crystal NMC materials by XPS, A. Dutta et al., Adv. Energy Mater., 15, e03051 (2025); DOI: 10.1002/aenm.202503051.
- Single-crystalline Ni-rich LiNixMnyCo1-x-yO2 cathode materials: a perspective, H. Zhang et al., Adv. Energy Mater., 12, 2202022 (2022); DOI: 10.1002/aenm.202202022.
Related Products