F HC Solar (CAS number 155090-83-8) is a water-based PEDOT:PSS formulation. F HC Solar is especially developed for applications in organic photovoltaics (OPVs), polymer and perovskite solar cells, and printed sensors. The main advantages of F HC Solar ink are its high conductivity and low contact angle, to improve the deposition on top of the active layer.

Increased Wettability F HC Solar PEDOT:PSS

Low Contact Angle

Improve the deposition on top of the active layer

Versatile use for OPV, OLED and perovskite solar cells

Versatile Use

Ideal for applications in OPV and perovskite solar cells

High quality PEDOT

High Quality

Quality formulation

High Conductivity PEDOT

Tailored Conductivity

High conductivity, >500 S/cm

Technical Data


Product Name Clevios™ F HC Solar
Solvent Water
Composition PEDOT/PSS
CAS Number 155090-83-8
Solid Content 1.0 – 1.5 wt.%
Work Function 4.8 – 5.0 eV
Resistivity <0.002 Ω/cm
Sheet Resistance 100 – 1000 Ω/sq
Conductivity High conductivity, >500 S/cm. Contact angle approx 10° (ITO), <30° (P3HT:PCBM)
Particle Size Distribution N/A
Viscosity 8 – 70 mPa.s
pH Value 1.0 – 2.0
Packaging 100 ml of solution sealed in a light resistant bottle with temperature indicator
Storage 3 – 5 °C

Spin Speed Data


F HC Solar Spin Speed / Film ThicknessF HC Solar Spin Speed / Film Thickness

MSDS Document


F HC Solar MSDS SheetF HC Solar PEDOT:PSS MSDS Sheet

Related Products


Resources


PEDOT:PSS Deposition How to Spin Coat PEDOT:PSS

For the deposition of thin films of PEDOT:PSS on a freshly prepared surface, we recommend using a vacuum-free spin coater and following this five-step process:

Read more...
PEDOT and PEDOT:PSS Synthesis PEDOT and PEDOT:PSS Synthesis

PEDOT synthesis involves the oxidative chemical or electrochemical polymerization of EDOT monomer. The choice of counterions and polymerization method significantly affects the conductivity, work function, and stability of the resulting PEDOT polymer.

Read more...

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message