PTB7-Th, also known as PCE10 or PBDTTT-EFT, is in the new generation of OPV donor polymers that could deliver on the heralded 10/10 target of 10% efficiency and 10 years lifetime. This material has already shown impressive potential with in excess of 9% efficiency reported in the literature and over 7% produced when using large area deposition processes in air with a standard architecture [1,2]. In our own labs we have achieved efficiencies of over 9%.
The advantages of PCE10 are that not only does the material lower HOMO/LUMO levels and increase the efficiencies compared to PTB7 but, more significantly, it is also far more stable. Early indications are that it can be handled under ambient conditions without issues, suggesting that we can look forward to measuring the long term lifetime of the devices.
The Luminosyn™ Range
High Purity Materials: Purified by Soxhlet extraction with methanol, hexane, and chlorobenzene under argon atmosphere.
Batch-Specific Data: Confidence in your materials with batch-specific GPC data for your thesis or publications.
Large Quantity Orders: Plan your experiments with confidence using polymers from the same batch.
Thienothiophene, Benzodithiophene, Heterocyclic five-membered ring, Organic semiconducting materials, Low band gap polymers, Organic Photovoltaics, Polymer Solar Cells, All-PSCs, NF-PSCs
Batch Details
Batch Number
MW
MN
PDI
Stock Info
M0261A6
135,141
53,926
2.51
In stock
Previous Batch Details
Batch Number
MW
Mn
PDI
Stock Info
M263
47,043
23,781
1.98
Discontinued
M264
57,467
27,395
2.10
Discontinued
M0261A1
56,484
22,733
2.48
Discontinued
M0261A3
57,183
29,285
1.95
Discontinued
M0261A4
125,205
47,538
2.63
Discontinued
M0261A5
133,198
61,416
2.17
Discontinued
Chemical Structure
PTB7-Th (PCE10) chemical structure, CAS No. 1469791-66-9
Applications
PCE10 is one of the most exciting materials to have made it out of the labs in recent years and offers huge potential for more in depth research. We'll be working hard over the next few months to maximize efficiencies by optimizing the device architecture, and we will provide further results as we do so. In the mean time, our current fabrication routine is below, and should you have any further questions or queries please contact us.
This fabrication routine was published in 2015 and used a now discontinued batch of PCE10, Batch No. M261, that had a broad range molecular weight definition of Mw > 40,000.
Reference devices were made on batch M261 to assess the effect of PBDTTT-EFT:PC70BM active layer thickness on OPV efficiency with the below structure. These were fabricated under inert atmosphere before encapsulation and measurement under ambient conditions.
Glass / ITO (100 nm) / PEDOT:PSS AI 4083 (30 nm) / PBDTTT-EFT:PC70BM (1:1.5) / Ca (5 nm) / Al (100 nm)
For generic details please see the fabrication guide and video. For specific details please see the below condensed fabrication report which details the optical modeling and optimization of the multilayer stack.
The PBDTTT-EFT:PC70BM solution was made in chlorobenzene (CB) at 35 mg/ml before being diluted with 3% diiodooctane (DIO) to promote the correct morphology.
Active layer thicknesses were achieved from spincasting the film at spin speeds of 2000, 2700, 3900 and 6000 rpm for 30s. Additionally, a methanol wash was performed for all devices to help remove the DIO additive. For each of these spin speeds a total of 2 substrates (3 in the case of 2700 rpm) was produced, each with 8 pixels and the data presented below represents a non-subjective (no human intervention) analysis of the best 75% of pixels by PCE (18 pixels for 2700 rpm condition, 12 pixels for each other).
Overall, the average efficiency of 8.30% PCE (9.01% maximum) was found from a 2700 rpm spin speed.
Figure 1: PCE, Jsc, Voc and FF for different spin speeds. Data shown is averaged with standard deviation of the best 75% of pixels. Standard deviation for Voc was ±0.01 V for each criterion. The JV curve (dark and under illumination) for the best performing device is shown below.
Note on effect of epoxy: Due to the very high solubility of the PBDTTT-EFT it was noted during fabrication that the film changed color when in contact with the encapsulation epoxy in liquid form for extended periods indicating that there was some miscibility. Inspection of the active areas underneath the top cathode indicated that the epoxy had not seeped into the active area before curing and device metrics indicate that this did not appear to affect performance. However, we would recommend minimizing contact time between the epoxy and PBDTTT-EFT films before UV curing.
Side Chain Selection for Designing Highly Efficient Photovoltaic Polymers with 2D-Conjugated Structure, S. Zhang et al., Macromolecules, 47, 4653-4659 (2014)
Highly Efficient 2D-Conjugated Benzodithiophene-Based Photovoltaic Polymer with Linear Alkylthio Side Chain, L. Ye et al., Chemistry of Materials., 26, 3603-3605 (2014)
Technical Support
We use essential cookies for core website functionality and collect anonymous, cookieless usage statistics. You can optionally allow analytics cookies to help us improve our site (more information)
Change Country
Change Currency
We were unable to change your currency due to a corrupted or expired cart cookie.
Click continue to delete your cart cookie and change your currency. This will remove all items from your cart. If this fails, please delete all cookies and try again, or contact us for further assistance.