Antimony tin oxide (CAS number 128221-48-7), also referred to as ATO, is a conducting metal oxide. Antimony tin oxide exhibits high transparency across the visible light spectrum (380–800 nm). When combined with self-assembled monolayer materials, antimony tin oxide is applied as an interlayer between perovskite and hole-transporting layers in an inverted perovskite solar cell. ATO improves the stability of the interface, suppresses non-radiative recombination, and enhances charge extraction in the solar cell. Such an inverted perovskite solar cell with ATO achieves a maximum power conversion efficiency (PCE) of 25.7%.

Antimony tin oxide decorated graphene (ATO/graphene) composite demonstrates high electrical conductivity and structural stability as an anode material in lithium batteries. ATO increases the lithium insertion rate and improves cycling stability, enabling the battery cells to reach a gravimetric capacity of 1226 mAh/g at 1C and 577 mAh/g at 60C. The ATO/graphene anode also shows excellent stability with a capacity retention of 77% after 1000 cycles.

Antimony tin oxide

Transparent metal oxide

as an electrode used in solar cells, OLEDs, and batteries

Antimony tin oxide

Antimony doped tin oxide

with doping level of 10%

Worldwide shipping

Quick and reliable shipping

High purity

High Purity

99.9%

General Information


CAS Number 128221-48-7
Chemical Formula SnO2:Sb2O3
Full Name Antimony tin oxide
Molecular Weight 164.32 g/mol (SnO2:Sb2O3 = 9:1)
Melting Point N/A
Synonyms ATO, Antimony doped tin oxide, Sb doped SnO2
Classification or Family Metal oxide, Conducting metal oxide, Batteries, Solar cells, Thermal management, Polymer composites

Product Details


Purity 99.9%
Particle Size 20 – 50 nm
Appearance Blueish gray powder

MSDS Documentation


Antimony Tin Oxide MSDS SheetAntimony Tin Oxide MSDS Sheet

References


  • Enhancing the efficiency and longevity of inverted perovskite solar cells with antimony-doped tin oxides, L. Jia et al., Nat. Energy, 9, 308–315 (2024); DOI: 10.1038/s41560-023-01442-1.
  • Flexible perovskite solar cells based on AgNW/ATO composite transparent electrodes, S. Jon et al., Syn. Met., 262, 116286 (2020); DOI: 10.1016/j.synthmet.2019.116286.
  • Utilizing the unique charge extraction properties of antimony tin oxide nanoparticles for efficient and stable organic photovoltaics, C. Liu et al., Nano Energy, 89, 106373 (2021); DOI: 10.1016/j.nanoen.2021.106373.


We stock a wide range of Metal Oxide available to purchase online. Please contact us if you cannot find what you are looking for.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message