PPCzTRz for High Efficiency and Stability Devices

Triplet-exciton-distributed (TED) TADF blue emitter


Specifications | MSDS | Literature and Reviews


PPCzTrz, or 9-(5'-(4,6-Diphenyl-1,3,5-triazin-2-yl)-[1,1':3',1''-terphenyl]-2'-yl)-3,6-diphenyl-9H-carbazole in full, is a TADF blue emitter. It has a typical D-π-A type structure consisting of an electron donating 3,6-diphenyl-9H-carbazole, an electron accepting 4,6-dipneyl-triazine, and a phenyl π linker inbetween. With two phenyl groups attached at meta-positions to each of the electron donating, accepting and π linker units, PPCzTrz is nonplanar with increased steric hindrance in structure to effectively weaken intermolecular forces.

By exploring two TADF materials, one distributing and one emitting, a triplet-exciton-distributed (TED) TADF device based on PPCzTrz as the assistant dopant and v-DABNA as the terminal emitter demonstrates:

  • A high external quantum efficiency of 33.5%
  • A color coordinate corrected current efficiency of 364 cd A–1
  • A long operational device lifetime (LT50, 50% of initial luminance) of 9500 h at 100 cd m–2
  • A y color coordinate below 0.10

The TED-TADF mechanism involves singlet excitons being transferred from the host to the emitter via the distributing TADF material by cascade energy transfer, whereas the triplet excitons are transferred to the emitter as singlet excitons by a triplet-exciton recycling process between the low-triplet-energy host and the distributing TADF material.

General Information


CAS Number 2329651-89-8
Full Name 9-(5'-(4,6-Diphenyl-1,3,5-triazin-2-yl)-[1,1':3',1''-terphenyl]-2'-yl)-3,6-diphenyl-9H-carbazole
Chemical Formula C57H38N4
Molecular Weight 778.94 g/mol
Absorption* λmax 444 nm in toluene
Fluorescence λem n.a.
HOMO/LUMO HOMO = 5.602 eV, LUMO = 2.657 eV
Classification or Family Carbazole, Triazine, TADF Blue Emitters, TED-TADF

Product Details


Purity >98.0% (1H NMR)
Melting Point Tg = 166 °C, Td = 466.3 °C
Appearance Yellow powder/crystals

Chemical Structure


PPCzTRz chemical structure
PPCzTRz (CAS 2329651-89-8) chemical structure

MSDS Documentation


PPCzTRz MSDS sheetPPCzTRz MSDS sheet

Literature and Reviews


  1. S. Jeon et al. (2021); High-efficiency, long-lifetime deep-blue organic light-emitting diodes, Nat. Photonics, 15, 208–215; DOI: 10.1038/s41566-021-00763-5.
  2. J. Wang et al. (2024); Promising interlayer sensitization strategy for the construction of high-performance blue hyperfluorescence OLEDs, Light Sci. Appl., 13, 139; DOI: 10.1038/s41377-024-01490-6.
  3. Y. Zhang et al. (2023); High-efficiency all fluorescence white OLEDs with high color rendering index by manipulating excitons in co-host recombination layers, Nanoscale, 15, 14249-14256; DOI: 10.1039/D3NR02568C.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message