It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

ITO Glass Substrate Pack, 20 x 15 mm, PV and OLED

Substrates and Fabrication

Product Code S213
Price $555

Create and Test 100 Fully Encapsulated Devices

Reduce edge ingress to improve device stability and maximize the volume of statistical data


Specifications | Related Products | Resources and Support


Substrate consumables for 100 fully encapsulated LEDs or PVs, suitable for measurement under ambient conditions. Designed for rapid fabrication, the substrate pack contains:

  • Pre-patterned ITO glass substrates (pack of 100)
  • Encapsulation epoxy (10 ml)
  • Encapsulation coverslips (pack of 100)
  • Electrical connection legs (200 strips of 6 legs)

Our substrates are manufactured from commercial-grade ITO used in the flat panel display industry for high consistency and very low defect rates. The encapsulation epoxy has been proven not to damage delicate polymers or reactive layers (such as calcium), and the encapsulation slips prevent water and oxygen ingress when storing your devices under ambient conditions. For testing, our electrical connection legs clip easily onto the sides of the substrate to make reliable contact with the ITO.


ITO photovoltaic substrate 3D exploded diagram (8 pixel)


We have discontinued our generation I and II substrates and masks. Contact us for help migrating to the new 8-pixel design.

Specifications


ITO Glass Substrates

Product Code S211
Substrate Size 20 mm x 15 mm
Thickness 1.1 mm
Glass Type Polished soda lime, float glass
Substrate Coating Fully oxidized ITO
ITO Thickness 100 nm
ITO Resistance 20 Ω/square
Glass Roughness < 1 nm RMS (by AFM)
ITO Roughness 1.8 nm RMS (by AFM)

Encapsulation Epoxy

Product Code E132
Viscosity 250 to 360 cps @ 23°C
Appearance Colorless
Cure Schedule 5 to 30 seconds at 250 to 350 nm at 10-100 mW/cm2
Refractive Index 1.4957 (at 589 nm)
Specific Gravity 1.09 to 1.21 g/cc
Cured Shore D Hardness 85+ D
Tensile Strength 8,000 psi
Elongation 3%
Glass Transition Temperature 138°C
CTE 50 x 10-6
Dielectric Constant 3.94 @ 60 Hz @ 20°C
Volume Resistivity 3.0 x 1014 Ω cm
Shelf Life 12 months at 23°C

Encapsulation Coverslips

Product Code C181
Size 12 mm x 15 mm
Thickness 0.55 mm
Material Float glass

Electrical Connection Legs

Product Code E242
Pitch 0.1 inch (2.54 mm)
For Glass Thickness 1.1 mm
Pack 200 x 6 legs

Resources and Support


Making OLEDs and OPVs: A Quickstart Guide

Organic photovoltaic cells (OPVs) or organic light emitting diodes (OLEDs) can be easily manufactured using Ossila's pre-patterned ITO substrates and a few simple spin coating and evaporating steps. This article, and its companion video, will guide you through this process and offer hints and tips for how to get the best devices.

Learn more...
transparent conductive oxides Transparent Conductive Oxides

Transparent conductive oxides (TCOs) are metal oxides, such as zinc oxide and tin oxide, that are capable of conducting electricity whilst being optically transparent. Find out about the chemistry behind ITO and why it is so popular.

Learn more...
Return to the top