Multi-Walled Carbon Nanotubes (MWCNT)


Product Code M2008D6-5g
Price $98

High Purity MWCNTs with Enhanced Strength and Durability

In powder form for applications to improve mechanical or electrical properties of materials


Product Information | MSDS | MWCNT Derivatives | Related Products | Technical Support


Multi-walled carbon nanotubes (MWCNTs), CAS number 308068-56-6, are a special form of carbon nanotubes in which multiple single-walled carbon nanotubes are nested inside one another. Their attractive mechanical, thermal and electrical properties are a result of their nanoscale tubular structure which consists of a hexagonal lattice of carbon atoms.

MWCNTs are exceptionally strong, with their multiple layers adding stiffness and durability. When used in a material composite they enhance toughness and reliability. MWCNTs are also useful for applications that benefit from increased dispersibility, and also enable reduced costs in synthesis and purification of these materials.

High Purity Multi-Walled Carbon Nanotubes

High Purity

>99% MWCNTs

Worldwide shipping for 308068-56-6

Worldwide Shipping

Quick and reliable shipping

Reduced cost in synthesis with 308068-56-6

Low Cost

Reduced cost in synthesis

Applications of Multi-Walled Carbon Nanotubes

Versatile Applications

Improve mechanical or electrical properties

General Information


CAS Number 308068-56-6
Chemical Formula CxHy
Recommended Dispersants DI Water, DMF, THF, Ethanol, Acetone
Synonyms Multi-Walled Carbon Nanotubes, Multi Wall Carbon Nanotube, Carbon Nanotube, MWNT, MWCNT
Classification or Family 1D materials, Carbon nanomaterials, Nanomaterials, Polycyclic aromatic hydrocarbons, thin-film electronics
Color and Appearance* Black fibrous powder

* All our MWCNTs come packed as dry powders, which can be dispersed within your solvent of choice.

Chemical Structure


Multi-walled carbon nanotubes, MWCNT
Multi-walled carbon nanotubes, MWCNTs, CAS number 308068-56-6

Product Details


Product code M2008D6 M2008D8 M2008S1
Internal Diameter (nm) 2 – 6 N/A N/A
Outer Diameter (nm) 4 – 8 10 – 30 10 – 30
Length (μm) 10 – 20 5 – 20 1 – 2
Specific Surface Area (m2/g) 330 120 – 170 120 – 170
Purity (%) > 96% 99% 99%

Dispersion Guide


Like single walled carbon nanotubes, MWCNT's are insoluble. For dispersing in aqueous solutions we recommend the use of sodium dodecylbenzene sulfonate if an ionic surfactant is suitable if a nonionic surfactant is needed we recommend surfactants with high molecular weights.

  • Weigh out the desired amount of nanotubes.
  • Mix together your solvent and surfactant of choice at the desired surfactant concentration. This should be below the critical micelle concentration of the surfactant.
  • Add the solvent-surfactant mix to the dry powder and shake vigorously to mix.
  • Either place an ultrasonic probe into the solution or place the solution into an ultrasonic bath. Be careful about the length of time and power used, as damage to the carbon nanotubes can occur, shortening their average length.
  • The resulting solution will be a mixture of suspended nanotubes and bundles of nanotubes, further sonication will help break up the bundles.
  • To separate out the individual nanotubes in solution from the bundles the solution should be placed within a centrifuge. If the solution is centrifuged for a longer time and/or at a higher the smaller bundles will be removed narrowing the distribution of suspended nanotubes.

For functionalized nanotubes it is possible to disperse them without the use of any surfactants. However, the total concentration of dispersed nanotubes will be lower.

MSDS Documents


Multi-walled carbon nanotube MSDSMulti-Walled Carbon Nanotube MSDS Sheet

References


  1. Thermal and Electrical Conductivity of Single and Multi-Walled Carbon Nanotube-Epoxy Composites, A Moisala et.al., Compos. Sci. Technol., 66, 1285-1288 (2006) DOI: 10.1016/j.compscitech.2005.10.016
  2. 99.9% Purity Multi-Walled Carbon Nanotubes by Vacuum High-Temperature Annealing, W. Huang, et. al., Carbon, 41, 2585-2590, (2003) DOI: 10.1016/S0008-6223(03)00330-0
  3. Elastic Moduli of Multi-Walled Carbon Nanotubes and the Effect of Van der Waals Forces, C. Li, et. al., 63, 1517-1524, (2003) DOI: 10.1016/S0266-3538(03)00072-1

MWCNT Derivatives


Multi-walled carbon nanotube derivatives have been developed in order to enhance specific properties. Functionalization of the MWCNT with COOH or OH chemical groups alters surface properties, improving the dispersibility of MWCNT in polar solvents. Nickel coated MWCNT have magnetic properties and graphene CNT composites have improved conductivity.


We stock a wide range of low dimensional materials available to purchase online. Please contact us if you cannot find what you are looking for.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message