Benzodithiophene-2THBr-4EH
Benzodithiophene-2THBr-4EH, high purity monomer for applications in OPVs and OFETs
For the synthesis of low band-gap polymer semiconductors
1,3-Bis(5-bromo-4-(2-ethylhexyl)thiophen-2-yl)-5,7-bis(2-ethylhexyl)benzo[1,2-c:4,5-c']dithiophene-4,8-dione, or Benzodithiophene-2THBr-4EH, is a monomer for the synthesis of low band-gap polymer semiconductors such as PBDD4T and PBDD4T-2F. It has applications in OPV (fullerene or fullerene-free), tandem organic solar cells, and OFETs.
Benzodithiophene-2THBr-4EH has a more soluble structure due to its four branched side chains, so resulting polymers can be more easily processed for device fabrications.
General Information
CAS number | 1439937-07-1 |
Chemical formula | C50H70Br2O2S4 |
Molecular weight | 991.16 g/mol |
Synonyms | 1,3-Bis(5-bromo-4-(2-ethylhexyl)thiophen-2-yl)-5,7-bis(2-ethylhexyl)benzo[1,2-c:4,5-c']dithiophene-4,8-dione |
Classification / Family | Thiophene, Fused thiophene, Benzodithiophene dione, Semiconductor synthesis intermediates, Low band gap polymers, OFETs, Organic photovoltaics, Polymer solar cells |
Product Details
Purity | > 98% (by 1H-NMR in CDCl3) |
Melting point | n/a |
Appearance | Yellowish-orange powder/crystals |
Chemical Structure

Characterisation

MSDS Documentation
Literature and Reviews
- A Fluorinated Polythiophene Derivative with Stabilized Backbone Conformation for Highly Efficient Fullerene and Non-Fullerene Polymer Solar Cells, S. Zhang et al., Macromolecules, 49 (8), 2993–3000 (2016); DOI: 10.1021/acs.macromol.6b00248.
- Achieving 12.8% Efficiency by Simultaneously Improving Open-Circuit Voltage and Short-Circuit Current Density in Tandem Organic Solar Cells, Y. Qin et al., Adv. Mater. 2017, 29, 1606340 (2017); DOI: 10.1002/adma.201606340.
To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, pharmaceuticals, cosmetics, food or commercial applications.