Graphitized Multi-Walled Carbon Nanotubes (G-MWCNT)
CAS Number 308068-56-6
Carbon Nanotubes (CNTs), Anode Active Materials, Inorganic Electronic Materials, Battery Materials,Graphitized Multi-walled Carbon Nanotubes (G-MWCNT) (-OH and -COOH functionalized)
High purity MWCNT annealed under inert gas at high temperature – used for applications in biosensors, drug delivery, catalytic reactions, supercapacitors, energy storage and batteries.
Specifications | Pricing and Options | MSDS | Literature and Reviews | Technical Support
Graphitized multi-walled carbon nanotubes (G-MWCNT), CAS number 308068-56-6, are multi-walled carbon nanotubes graphitized by annealing under inert gas at high temperatures. The graphitization procedure can remove residual metal catalyst in the nanotubes and reduce the wall defects. High purity over 99.9% can be achieved by the annealing process however the the graphitization process is also known to reduce the specific surface area by half.
Graphitized carbon nanotubes thus can be considered as a new hybrid of graphitic foliates grown along the sidewalls of multi-walled carbon nanotubes (CNTs). The high temperature thermal treatment produces multi-walled carbon nanotubes with the highest graphite crystallization, electrical conductivity, and the best oxidation resistance.
Aluminum-Graphitic MWCNT cell with graphitic MWCNT serves as an active cathode for rechargeable Al-ion battery exhibits good electrochemical performance with a specific capacity of 64 mAh·g-1 at a current density of 200 mA·g-1, and delivers 58 mAh·g-1 with ~100% retention over 1000 cycles. Graphitized carbon nanotubes also finds applications in the following areas:
- Biosensors
- Electrodes for batteries and supercapacitors
- Hydrogen storage
- Flat panel displays
- Transistor
- Catalysis
- Drug delivery
Reduced wall defects
Graphitization purifies the MWCNTs
Various Applications
Used in batteries, hydrogen storage, transistors, catalysis, biosensers and drug delivery
Worldwide shipping
Quick and reliable shipping
High purity
>99.9% High purity
General Information
| CAS Number | 308068-56-6 |
|---|---|
| Chemical Formula | CxHyOz |
| Full Name | Graphitized Multi-walled Carbon Nanotubes |
| Synonyms | G-MWCNT, Graphitized MWCNT |
| Classification / Family | Graphite, Carbon Nanotubes, 1D Materials, Carbon Nanomaterials |
| Appearance | Black powder |
Product Detail
| Product Code | M2374A1 | M2374B1 | M2374C1 |
|---|---|---|---|
| Purity | >99.9% | >99.99% | >99.99% |
| External Diameter (nm) | 28 – 48 | 28 – 48 | 28 – 48 |
| Size (μm) | 5 – 10 | 10 – 30 | 10 – 30 |
| Function Group | N/A | OH | COOH |
| Function Group Content | N/A | 0.55 wt% | 0.35 wt% |
| Electrical Conductivity (s/cm) | 98 | 98 | 98 |
| Surface Area (m2/g) | 35 | 35 | 35 |
| Synthetic Method | CVD | CVD (at 800 ℃) | CVD (at 800 ℃) |
Pricing
| Batch | Quantity | Price |
|---|---|---|
| M2374A1 | 5 g | £280 |
| M2374A1 | 10 g | £460 |
| M2374B1 | 1 g | £115 |
| M2374B1 | 5 g | £460 |
| M2374C1 | 1 g | £115 |
| M2374C1 | 5 g | £460 |
MSDS Documentation
Graphitized Multi-walled Carbon Nanotubes (G-MWCNT) MSDS Sheet
Graphitized Multi-Walled Carbon Nanotubes OH functionalized MSDS Sheet
Graphitized Multi-Walled Carbon Nanotubes COOH functionalized MSDS Sheet
Literature and Reviews
-
Purification and structural annealing of multiwalled carbon nanotubes at graphitization temperatures, R. Andrews et al., Carbon, 39 (11), 1681-1687 (2001); DOI: 10.1016/S0008-6223(00)00301-8.
-
Graphitic multi-walled carbon nanotube cathodes for rechargeable Al-ion batteries with well-defined discharge plateaus, M. Han et al., J. Power Sources, 451, 227769 (2020); DOI: 10.1016/j.jpowsour.2020.227769.
-
99.9% purity multi-walled carbon nanotubes by vacuum high-temperature annealing, W. Huang et al., Carbon 41. 2585–2590 (2003); DOI: 10.1016 / S0008-6223(03)00330-0.