It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M621-250mg
Price $210

m-MTDATA, effective HIL material to lower driving voltage of OLED devices

Available online for priority dispatch,  4,4',4''-Tris[phenyl(m-tolyl)amino]triphenylamine, CAS No. 124729-98-2, Sublimed ≥99.0%


Overview | Specifications | Pricing and Options | MSDS | Literature and Reviews


With its very low solid-state ionisation potential and good-quality amorphous film, 4,4',4''-Tris[phenyl(m-tolyl)amino]triphenylamine, m-MTDATA acts as an effective material for the hole-injection buffer layer (HIL) that facilitates hole injection from the ITO electrode to the hole transporting layer (HTL). This potentially lowers the driving voltage of the OLED devices.

F4-TCNQ, a strong electron acceptor, is always used together with m-MTDATA as a p-doping material to improve the conductivity of the HTL buffering layer. Typical structure of the device (or part of the device) is ITO/p-doped m-MTDATA/HTL/etc.

General Information


CAS number 124729-98-2
Chemical formula C57H48N4
Molecular weight 789.02 g/mol
Absorption λmax 312 nm, 342 nm in THF
Fluorescence λem 425 nm in THF
HOMO/LUMO HOMO 5.1 eV, LUMO 2.0 eV [1]
Synonyms 4,4',4''-Tris[(3-methylphenyl)phenylamino]triphenylamine
Classification / Family Triphenylamine derivatives, Hole-injection materials, Hole transporting materials, Light-emitting diodes, Organic electronics

Product Details


Purity Sublimed* >99.0% (HPLC)
Melting point 210 °C
Appearance Yellow/white powder

*Sublimation is a technique used to obtain ultra pure-grade chemicals. For more details about sublimation, please refer to the Sublimed Materials.

Chemical Structure


m-mtdata, 124729-98-2
Chemical Structure of 4,4′,4′′-Tris[phenyl(m-tolyl)amino]triphenylamine (m-MTDATA), CAS 124729-98-2

Device Structure(s)


Device structure ITO/MoOx (2 nm)/m-MTDATA: MoOx (30 nm, 15 wt.%)/m-MTDATA
(10 nm)/Ir(ppz)3 (10 nm)/CBP:PO-01* (3 nm, 6 wt.%)/Ir(ppz)3
(1 nm)/DBFDPOPhCz*:FIrpic (10 nm,10 wt.%)/Bphen (36 nm)/LiF
(1 nm)/Al [3]
Colour White white light emitting device
Max. EQE 12.2%
Max. Current Efficiency 42.4 cd/A
Max. Power Efficiency 47.6 lm W−1
Device structure ITO/[F4-TCNQ(x nm)/m-MTDATA(y nm)]n/NPB/Alq3/Bphen/Cs2CO3/Al [4]
Colour Green green light emitting device
Max. Luminance 23,500 cd/m2
Max. Current Efficiency 7.0 cd/A
Max. Power Efficiency 4.46 lm W−1
Device structure ITO/PEDOT:PSS AI 4083(40nm)/m-MTDATA:Ir(Flpy-CF3)3 (40nm)/TmPyPB(55nm)/LiF(0.5nm)/Al(100nm) [5]
Colour Yellow yellow device
Max. EQE 25.2%
Max. Luminance 43,085 cd/m2
Max. Current Efficiency 74.3 cd/A
Max. Power Efficiency 97.2 lm W−1
Device structure ITO/PEDOT:PSS/m-MTDATA (20 nm)/m-MTDATA:3TPYMB (60 nm)/3TPYMB (10 nm)/LiF (0.8 nm)/ Al (100 nm) [6]
Colour Red red light emitting device
Max. Luminance 17,100cd/m2
Max. Current Efficiency 36.79 cd/A
Device structure ITO (80 nm)/m-MTDATA (20 nm)/NPB (20 nm)/[ADN:Alq3 (4:1)]:1wt.% DCJTB:0.2wt.%C545T/Alq3 (30 nm)/LiF (1 nm)/Al (100 nm) [7]
Colour Red red light emitting device
Max. Luminance 11,600 cd/m2
Max. Current Efficiency 3.6 cd/A
Device structure ITO/m-MTDATA*:F4-TCNQ (100 nm)/TPD (5 nm)/Alq3 (20 nm) /BPhen (10 nm)/ Bphen:Li (30 nm)/LiF (1 nm)/Al (100 nm) [8]
Colour Green green light emitting device
Max. Luminance 10,000 cd/m2 at 5.2 V
Max. Current Efficiency 5.27 cd/A
Device structure ITO/m-MTDATA (30 nm)/NPB (20 nm)/TPBI:4 wt% Ir(ppy)3:2 wt%Ir(piq)2(acac) (30 nm)/Alq3(20 nm)/LiF/Al [9]
Colour White white light emitting device
Max. Luminance 33,012 cd/m2
Current Efficiency@100 cd/m2 15.3 cd/A
Max. Powder Efficiency 10.7 lm W−1
Device structure ITO/m-MTDATA/TPD/F-TBB*/Alq3/MgAg [10]
Colour Blue blue light emitting device
Max EQE 1.4%
Maximum luminance 3960 cd m-2 at 15.0 V

*For chemical structure information please refer to the cited references.

Pricing


Grade Order Code Quantity Price
Sublimed (>98.0% purity) M621 250 mg £155
Sublimed (>98.0% purity) M621 500 mg £250
Sublimed (>98.0% purity) M621 1 g £420

MSDS Documentation


m-MTDATA MSDSm-MTDATA MSDS sheet

Literature and Reviews


  1. Nanoscale transport of charge-transfer states in organic donor–acceptor blends, P. B. Deotare et al., Nat. Mater., 14, 1130-1135 (2015). DOI: 10.1038/NMAT4424.
  2. Photophysical Investigation of the Thermally Activated Delayed Emission from Films of m-MTDATA:PBD Exciplex, D. Graves et al., Adv. Funct. Mater., 24, 2343–2351 (2014). DOI: 10.1002/adfm.201303389.
  3. Highly efficient and color-stable white organic light-emitting diode based on a novel blue phosphorescent host, Q. Wu et al., Syn. Metals 187, 160– 164 (2014). http://dx.doi.org/10.1016/j.synthmet.2013.11.010.

Return to the top