Product Code M0521A4-100mg
Price $338

PolyTPD, excellent HTL material for photovoltaics

High quality polymer available with free shipping on qualifying orders


Specifications | MSDS | Literature and Reviews


Poly(N,N'-bis-4-butylphenyl-N,N'-bisphenyl)benzidine, also known as polyTPD or Poly-TPD (CAS number 472960-35-3), is an excellent hole transport layer material used in photovoltaics such as perovskite solar cells. It has also proven polyTPD is a promising HTL candidate in multilayer WPLEDs because its HOMO level 5.2 eV is very close to the work function of the indium tin oxide ITO/PEDOT:PSS anode.

Ossila's PolyTPD was used in a high-impact paper (IF 13.281)

PolyTPD from Ossila was used in the high-impact paper (IF 13.281), Self-Powered Low-Cost UVC Sensor Based on Organic-Inorganic Heterojunction for Partial Discharge Detection, T. Park et al., Small, 2100695 (2021); DOI: 10.1002/smll.202100695.

As the highest occupied molecular orbital (HOMO) of polyTPD matches well with the VB of the perovskite, which allows for a good transport of holes towards the polyTPD, it is a popular semiconducting material candidate that is used in the HTL of the perovskite structures. And also as the LUMO of polyTPD is significantly closer to vacuum compared with that of the perovskite CB, polyTPD efficiently blocks the flow of electrons [5].

Like PTAA, polyTPD is one of the family members of poly(triaryl)amines.

General Information


CAS Number 472960-35-3
Chemical Formula (C22H21N)n
HOMO / LUMO HOMO 5.2 eV LUMO 2.3 eV [1]
Soluble in THF, o-xylene, toluene, chloroform, chlorobenzene
Recommended Processing Solvents at 10mg/ml Toluene (8mg/ml)
Synonyms

Poly[N,N’-bis(4-butylphenyl)-N,N’-bisphenylbenzidine]

Poly(4-butylphenyldiphenylamine)

polytpd

poly-tpd

Classification / Family Poly(triarylamines), Organic semiconducting materials, Hole transport layer materials (HTL), Electron block layer material (EBL), Organic Photovoltaics, Polymer Solar Cells, Light-emitting Diodes, Quantun Dot Light-emitting Diodes, OFETs and Perovskite hole transport layer materials

Batch information


Batch number MW Mn PDI Stock info
M0521A4 19,345 7,620 2.54 Low stock
M0521A5 63,630 11,915 5.34 In stock

Chemical Structure


Chemical structure of PolyTPD
Chemical structure of PolyTPD

Device Structure(s)


Device Structure ITO/PEDOT:PSS/PVK:polyTPD (1:1 wt%) 50 nm/PFO:MEH-PPV*(95.5:0.5 wt%) 70 nm/Ca/Al [4]
Colour white light emitting device White
Max. Luminance ~ 5,000 cd/m2
Max. Current Efficiency 3.15 cd/A
Device Structure ITO/P(VDF-TrFE-CFE) (1000 nm)/poly-TPD:F4TCNQ (7%, 70 nm)/ PVK:OXD-7:Ir(ppy)3 (150 nm)/TmPyPB(40 nm)/LiF(1 nm)/Al(150 nm) [7]
Colour green light emitting device Green
Max. Luminance 13,800 cd/m2
Max. Current Efficiency 76.2 cd/A
Max. Power Efficiency 17.1 lm W−1
Device Structure ITO/PEDOT:PSS(30 nm)/poly-TPD(40 nm)/DNA-CTMA*(20 nm)/PFO:MEH-PPV (70 nm)/Cs2CO3(1 – 2 nm)/Al [2]
Colour white light emitting device White
Max. Luminance 10,500 cd/m2
Max. Current Efficiency 10 cd/A

*For chemical structure informations please refer to the cited references

Device Structure ITO/polyTPD/CH3NH3PbI3/PCBM/C60/BCP/Ag [6] ITO/PEDOT:PSS/CH3NH3PbI3/PCBM/C60/BCP/Ag [6]
JSC (mA cm-2) 22.0 11.3
VOC (V) 1.0 (1.1a) 0.79
FF (%) 69.7 62.7
PCE (best) 15.3 5.58

PolyTPD as a HTL to compare with PEDOT:PSS a) 1.0 V in the supporting information and 1.1 V in the body text of the cited lit. [6]

MSDS Documentation


PolyTPD MSDS SheetPolyTPD MSDS Sheet

Literature and Reviews


  1. Bright, multicoloured light-emitting diodes based on quantum dots, Q. Sun et al., Nat. Photonics, 1, 717 - 722 (2007); doi:10.1038/nphoton.2007.226.
  2. Multilayer white polymer light-emitting diodes with deoxyribonucleic acid-cetyltrimetylammonium complex as a hole-transporting/electronblocking layer, Q. Sun et al., Appl. Phys. Lett., 92, 251108 (2008); doi: 10.1063/1.2948864.
  3. Electro-optics of perovskite solar cells, Q. Lin et al., Nat. Photonics, 9, 106–112 (2015); doi:10.1038/nphoton.2014.284.

Return to the top