It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


High quality platinum plate electrode

Use as an auxiliary/counter electrode and anode or cathode in electrochemistry


Overview | Specifications | Pricing and Options


Platinum plate electrodes can usually be used as auxiliary/counter electrodes for various electrochemical measurements as the three-electrode system for cyclic voltammetry and linear sweep voltammetry studies. They can also be used as an anode or cathode.

With remarkable resistance to corrosion, platinum (Pt) is naturally one of the least reactive metals therefore it is normally the first choice for both the working and counter electrodes. Unlike a platinum wire counter electrode, the platinum plate electrode can increase its surface area for electrochemical studies that require a larger surface area to match and support the current generated on the working electrode in any chemical reactions.

Due to platinum plate electrode’s resistance to oxidation, it is an excellent choice for anode in several electrochemical processes, such as the electrolysis of an acetate salt to give ethane and carbon dioxide. Anodic oxidation of benzene on a platinum electrode in the presence of BF3·OEt2 gives flexible, highly conducting films of Poly(p-phenylene) (PPP). Platinum and platinum-based alloys are also used as one of the most active cathode materials for oxygen reduction reaction (ORR) both in acid and alkaline solutions.

Large Surface Area

For optimized surface-to-working electrode ratio

High Quality

High Quality Materials

Industry Standard

Inert electrode with low catalytic activity

Expert Support

From in-house scientists & our
customer care team

Buy the platinum plate electrode together with reference electrode, working electrode, electrochemical cell and our Ossila potentiostat for a complete package to start your electrochemical studies.

Specifications


All dimensions are in millimeters.

Platinum Plate Working Electrode Dimensions
Platinum Plate Working Electrode Dimensions (mm)
Plate Dimension 10 x 10 x 0.1 mm

Pricing and Options


Product Name Product Code Price
Platinum Plate Working Electrode - 10 x 10 x 0.1 mm C2013N1 £320

Learn More


Cyclic Voltammetry Basics, Setup, and Applications Cyclic Voltammetry Basics, Setup, and Applications

Cyclic voltammetry is an electrochemical technique for measuring the current response of a redox active solution to a linearly cycled potential sweep between two or more set values.

Read more...
Linear Sweep Voltammetry: Introduction and Applications Linear Sweep Voltammetry: Introduction and Applications

Linear sweep voltammetry (LSV) is a simple electrochemical technique. The method is similar to cyclic voltammetry, but rather than linearly cycling over the potential range in both directions, linear sweep voltammetry involves only a single linear sweep from the lower potential limit to the upper potential limit.

Read more...

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message