DTY6, developed for large-area organic solar cells
Highly efficient non-fullerene acceptor from the Y6 family, available for priority dispatch
Specifications | Pricing and Options | MSDS | Literature and Reviews
DTY6 is another highly efficient non-fullerene acceptor from the Y6 family with a highly conjugated and flat [1,2,5]thiadiazolo[3,4-e]thieno[2",3’':4’,5']thieno[2',3':4,5]pyrrolo[3,2-g]thieno[2',3':4,5]thieno[3,2-b]indole core centre.
Bearing two large decylteradecyl alky side chains, DTY6 is developed for large-area organic solar cells. Working together with polymers PBDB-TF-T1 (T1), PTO2, PClTO2. Non-fullerene acceptors DTY6, BTP-2F-12, TPT10-C8C12 and BTP-eC9 are considered to be green energy materials for their green solvents processability, i.e. in o-xylene or THF.
High efficient non-fullerene acceptor
With highly conjugated core
Enhanced solubility
With decylteradecyl alkyl chains
Worldwide shipping
Quick and reliable shipping
Green energy materials
Processable in non-halogenated solvents
Polymer organic solar cells based on PM6:DTY6 processed in non-halogenated solvent o-xylene achieved power conversion efficiency of 16.1% with the following simple structure.
Device structure: (ITO)/PEDOT:PSS AI 4083/PM6:DTY6 (1:1.2, w/w, polymer weight concentration of 8 mg/mL)/PFN-Br/Ag. [1]
Thickness (nm) | VOC (V) | JSC (mA cm-2) | FF (%) | PCEmax (%) |
110 ± 20 nm | 0.848 | 25.3 | 75.1 | 16.1 |
General Information
CAS Number | N/A |
Chemical Formula | C114H150F4N8O2S5 |
Purity | >99% (1H NMR) |
Full Name | 2,2'-((2Z,2'Z)-((12,13-bis(2-decylteradecyl)-3,9-diundecyl-12,13-dihydro-[1,2,5]thiadiazolo[3,4-e]thieno[2",3’':4’,5']thieno[2',3':4,5]pyrrolo[3,2-g]thieno[2',3':4,5]thieno[3,2-b]indole-2,10-diyl)bis(methanylylidene))bis(5,6-difluoro-3-oxo-2,3-dihydro-1H-indene-2,1-diylidene))dimalononitrile |
Molecular Weight | 1900.83 g/mol |
HOMO / LUMO | HOMO = -5.67 eV, LUMO = -4.04 eV [1] |
Absorption | λmax 716 nm (in o-xylene), 836 nm (in o-xylene processed film) |
Synonyms | BTP-4F-24, Y6-DT |
Classification / Family | NFAs, n-type non-fullerene electron acceptors, Organic semiconducting materials, Low band-gap small molecule, Small molecular acceptor, Organic photovoltaics, Polymer solar cells, NF-PSCs. |
Chemical Structure

Pricing
Batch | Quantity | Price |
M2274A1 | 50 mg | £210 |
M2274A1 | 100 mg | £360 |
M2274A1 | 250 mg | £720 |
M2274A1 | 500 mg | £1290 |
MSDS Documentation
Literature and Reviews
- Single-Component Non-halogen Solvent-Processed High-Performance Organic Solar Cell Module with Efficiency over 14%, S. Dong et al., Joule 4 (9), 2004-2016 (2020); DOI: 10.1016/j.joule.2020.07.028.
Related Products
Semiconducting polymers for bulk heterojunction, OPV, OLED, OFET and perovskite interfaces and solar cell research.