It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

Spiro-OMeTAD (Spiro-MeOTAD)


Product Code M292-500mg
Price $450

High Performance Hole Transport Layer Material

With excellent electronic properties and processability for solar cells and OLEDs


Specifications | MSDS | Pricing | Literature | Related Products | Technical Support


Spiro-OMeTAD (or Spiro-MeOTAD) is one of the most studied and suitable hole transport layer materials due to its facile implementation and high performance in organic-inorganic electronic devices. The spiro-linked molecule provides high glass transition temperature (Tg), morphological stabilit, and easy processability, while maintaining good electronic properties. Widely used in solid-state dye-sensitized solar cells, organic light-emitting diodes, perovskite solar cells, and polymer-based organic solar cells, it is an ideal choice across many areas of research.

High-purity Spiro-OMeTAD in useful quanities is in stock for immediate dispatch with worldwide delivery. Please contact us for bulk orders over 100 g.

Ossila's Spiro-OMeTAD was used in a high impact paper (IF 29.37)

Spiro-OMeTAD from Ossila was used in the high-impact papers (IF 29.37), Interfacing Pristine C60 onto TiO2 for Viable Flexibility in Perovskite Solar Cells by a Low-Temperature All-Solution Process, Y. Zhou et al., Adv. Energy Mater., 1800399 (2018); and (IF 39.714), In situ simultaneous photovoltaic and structural evolution of perovskite solar cells during film formation, M. Alsari et al., Energy Environ. Sci., 11, 383-393 (2018).

Spirobifluorene hold transport layer material

Spirobifluorene HTL Material

Facile implementation & high performance in electronic devices

207739-72-8 Worldwide shipping

Simple Worldwide Shipping

Reliable delivery via tracked
courier as standard

High glass transition temperature and morphological stability

Ideal for Facile Coupling Reactions

High glass transition temperature
and morphological stability

High purity 207739-72-8

High Purities Available

Guaranteed 99.5% (sublimed)
and 99% (unsublimed)

General Information


CAS Number 207739-72-8
Molecular Formula C81H68N4O8
Full Name 2,2',7,7'-Tetrakis[N,N-di(4-methoxyphenyl)amino]-9,9'-spirobifluorene
Synonyms

Spiro-MeOTAD

Mw 1225.43 g/mol
UV Absorption Max 306 nm, 385 nm (in CH2Cl2)
PL Max 429 nm (in CH2Cl2)
HOMO / LUMO HOMO = -5.0 eV, LUMO = -2.05 eV (HOMO - Eg)
Eg (optical) 2.95 eV

Chemical Structure


Spiro-MeOTAD, 207739-72-8
Spiro-OMeTAD chemical structure, CAS 207739-72-8

Product Details


Purity

Sublimed: >99.5% (HPLC)

Unsublimed: >99.0% (HPLC)

Melting Point 240 °C (approx.)
TGA >360 °C (0.5% weight loss)
Appearance White to pale yellow powder

*Sublimation is a technique used to obtain ultra pure-grade chemicals. For more details about sublimation, please see our collection of sublimed materials .

Characterization


Spiro-OMeTAD HPLC trace
HPLC trace and 1H-NMR spectrum for Spiro-OMeTAD with > 99.5% purity.

MSDS Document


Spiro-OMeTAD MSDS SheetSpiro-OMeTAD MSDS Sheet

Pricing


Unsublimed

Product Code Purity Quantity Price
M291 >99.0% purity 500 mg £210
1 g £350
5 g £1560
10 g £2500

Sublimed

Product Code Purity Quantity Price
M292 Sublimed (>99.5% purity) 500 mg £300
1 g £480
5 g £2100
10 g £4000

References


  1. Interface engineering of highly efficient perovskite solar cells, Huanping Zhou et al., Science, V 34, p.546 (2014).
  2. Sequential deposition as a route to high-performance perovskite-sensitized solar cells, Julian Burschka et al., Nature, V499 p.316 (2013).
  3. Nanostructured TiO2 /CH3NH3PbI3 heterojunction solar cells employing spiro-OMeTAD/Co-complex as hole-transporting material, Jun Hong Noh et al., J. Mater. Chem. A, 1, 11842-11847, DOI: 10.1039/C3TA12681A (2013).

Related Products


Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message