It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M2050A1-100mg
Price $594

PBDD4T-2F, for highly efficient OPV devices

High purity and available online for priority dispatch


Specifications | MSDS | Literature and Reviews


PBDD4T-2F (CAS number 1890205-85-2) polymer semiconductor has been developed for OPV applications (including both fullerene and non-fullerene polymer solar cells) and has an efficiency of over 9% [1]. It has been built into tandem solar cells, and PCE reaching 13% was reported with the following structure: PBDD4T-2F:PC71BM (front cell) & PBDTTT-E-T:IEICO (rear cell) [2].

When compared to PBDD4T, PBDD4T-2F has a stronger tendency to aggregate in solution. It also has a stronger π–π stacking compact in solid thin-film, and shows a deeper HOMO energy level of -5.39 eV.

PBDD4T-2F finds applications in polymer solar cells with both fullerene and non-fullerene acceptors (such as ITIC and P(NDI2OD-T2) respectively) with highly efficient device performances.

Please enquire for 5-10 grams order quantity, the lead time is 4-6 weeks.

Luminosyn™ PBDD4T-2F


Luminosyn™ PBDD4T-2F is now available.

High purity and high molecular weight

PBDD4T-2F is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere - polymer at its pure best

Batch-specific GPC data

Have confidence in what you are ordering; batch-specific GPC data for your thesis or publications

Large quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


Full name Poly[[5,​7-​bis(2-​ethylhexyl)​-​4,​8-​dioxo-​4H,​8H-​benzo[1,​2-​c:4,​5-​c']​dithiophene-​1,​3-​diyl]​[3,​3'''-​bis(2-​ethylhexyl)​-​3'',​4'-​difluoro[2,​2':5',​2'':5'',​2'''-​quaterthiophene]​-​5,​5'''-​diyl]​]
Synonyms BDD4T-2F, PBDD-ff4T
Chemical formula (C58H72F2O2S6)n
CAS number 1890205-85-2
HOMO / LUMO HOMO = -5.39 eV, Eg = 1.76 eV [1]
Classification / Family Polythiophenes, Organic n-type semiconducting materials, Organic Photovoltaics, Polymer solar cells, Tandem Solar Cells, Electron-acceptor polymers, OFETs, Perovskite solar cells, All-polymer solar cells.
Soluble in  Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml

Dichlorobenzene or Chlorobenzene+dichlorobenzene (1:1 v/v) at elevated temperature ca. 80 °C

Batch details


Batch Mw Mn PDI Stock Info
M2050A1 138,330 53,285 2.60 In Stock

Chemical Structure


pbdd4t-2f, chemical structure
Chemical structure and product image of PBDD4T-2F

MSDS Documentation


PBDD4T-2F MSDSPBDD4T-2F MSDS Sheet

Literature and Reviews


  1. A Fluorinated Polythiophene Derivative with Stabilized Backbone Conformation for Highly Efficient Fullerene and Non-Fullerene Polymer Solar Cells, S. Zhang et al., Macromolecules, 49 (8), 2993–3000 (2016); DOI: 10.1021/acs.macromol.6b00248.
  2. Achieving 12.8% Efficiency by Simultaneously Improving Open-Circuit Voltage and Short-Circuit Current Density in Tandem Organic Solar Cells, Y. Qin et al., Adv. Mater., 29, 1606340 (2017); DOI: 10.1002/adma.201606340.
  3. Over 11% Efficiency in Tandem Polymer Solar Cells Featured by a Low-Band-Gap Polymer with Fine-Tuned Properties, Z. Zheng, Adv. Mater., 28, 5133–5138 (2016); DOI: 10.1002/adma.201600373.
Return to the top