HTL Solar 3 PEDOT Complex
Materials, Organic Conductors, PEDOT Polymer BlendsToluene-Based PEDOT Formulation
Used for applications in OPV and perovskite solar cells
Specifications | MSDS | Resources and Support
The future production of HTL Solar 3 PEDOT Complex has been discontinued. We can only supply HTL Solar 3 PEDOT Complex as stock lasts. It will be replaced by HTL Solar 4 PEDOT (M1214) Complex in anisole as an alternative with similar properties.
HTL Solar 3 PEDOT Complex is a toluene-based PEDOT formulation using an alternative counter ionomer to PSS, allowing for the dispersion in toluene. HTL Solar 3 is ideal for use with materials, or in environments, that are water sensitive. Examples include in glove box environments or for use with perovskite inks or perovskite precursor materials.
Increased Wettability
Ideal for perovskite solar cells or with materials dissolved in or degraded by water.
Versatile Use
Ideal for use with water sensitive materials or environments
High quality
Quality formulation
Low Conductivity
Low conductivity 0.002 – 0.2 S/cm
PEDOT Complex (HTL Solar 3) from Ossila was featured in the high-impact paper (IF 39.8), Efficient, stable, and fully printed carbon-electrode perovskite solar cells enabled by hole-transporting bilayers, T. Du et al., Joule, 7 (8), 1920-1937 (2023); DOI: 10.1016/j.joule.2023.06.005; and paper (IF 22.0), Carbazole-Based Hole Transport Polymer for Methylammonium-Free Tin–Lead Perovskite Solar Cells with Enhanced Efficiency and Stability, J. Wang et al., ACS Energy Lett., 7 (10), 3353–3361 (2022); DOI: 10.1021/acsenergylett.2c01578.
Technical Data
Product Name | Clevios™ HTL Solar 3 |
---|---|
Solvent | Toluene |
Composition | PEDOT complex |
Solid Content | 1.5 – 2.5 wt.% |
Work Function | 4.4 – 4.8 eV |
Resistivity | 5 – 500 Ω/cm |
Sheet Resistance | +10E6 Ω/sq |
Conductivity | Low conductivity 0.002 – 0.2 S/cm |
Particle Size Distribution | N/A |
Viscosity | <30 mPa.s |
pH Value | N/A |
Packaging | 2 x 25 ml of solution sealed in light resistant bottles with temperature indicators |
Storage | 3 – 5 °C |
Spin Speed Data
HTL Solar 3 Spin Speed / Film Thickness
MSDS Document
HTL Solar 3 PEDOT Complex MSDS Sheet
Related Products
Resources and Support

For the deposition of thin films of PEDOT materials on a freshly prepared surface, we recommend using a vacuum-free spin coater and following this five-step process:
Read more...PEDOT synthesis involves the oxidative chemical or electrochemical polymerization of EDOT monomer. The choice of counterions and polymerization method significantly affects the conductivity, work function, and stability of the resulting PEDOT polymer.
Read more...