Non-Aqueous Butyl Benzoate Based Blue PEDOT Complex Dispersion

Used for applications in HIL, printed OLED/QLED, and displays


Specifications | MSDS | Resources and Support


HIL 8 PEDOT Complex is a pH neutral non-aqueous butyl benzoate based blue PEDOT complex dispersion, with an alternative counter ionomer of PSEBS. HIL 8 PEDOT Complex is designed as hole injection layer material (HIL) for OLEDs, OPVs, and perovskite solar cells.

Deep Work Function PEDOT

Deep Work Function

Matching interfacial energy levels

Versatile HIL 8 PEDOT Complex

Versatile use

Ideal for applications in HIL, printed OLED/QLED, and displays

High quality PEDOT

High Quality

Quality formulation

Low conductivity

Tailored Low Conductivity

Low conductivity

Technical Data


Product Name Clevios™ HIL 8
Solvent Butyl benzoate
Composition PEDOT complex
Solid Content 3.0 – 4.0 wt.%
Work Function 5.0 – 5.1 eV
Resistivity 100 – 10000 Ω/cm
Sheet Resistance +10E6 Ω/sq
Conductivity Low conductivity
Particle Size Distribution N/A
Viscosity 5 – 9 mPa.s
pH Value pH neutral
Packaging 25 ml of solution sealed in a light resistant bottle with temperature indicator
Storage 3 – 5 °C

Spin Speed Data


P JET (OLD) Spin Speed / Film ThicknessHIL 8 Spin Speed / Film Thickness

MSDS Document


HIL 8 MSDS SheetHIL 8 PEDOT Complex MSDS Sheet

Related Products


Resources


PEDOT:PSS Deposition How to Spin Coat PEDOT Materials

For the deposition of thin films of PEDOT materials on a freshly prepared surface, we recommend using a vacuum-free spin coater and following this five-step process:

Read more...
PEDOT and PEDOT:PSS Synthesis PEDOT and PEDOT:PSS Synthesis

PEDOT synthesis involves the oxidative chemical or electrochemical polymerization of EDOT monomer. The choice of counterions and polymerization method significantly affects the conductivity, work function, and stability of the resulting PEDOT polymer.

Read more...

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message