It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M2249A1-100mg
Price $446

BTP-eC9, Y series n-type non-fullerene acceptor with NIR absorption

Available to buy online or request a quote today and enjoy discounts on large quantities


Specifications | Pricing and Options | MSDS | Literature and Reviews


BTP-eC9 (CAS number 2598965-39-8) is a family member of the Y series of n-type non-fullerene semiconducting acceptors. It has been proven that these NFAs can achieve high device performance in non-fullerene polymer solar cells (NF-PSCs).

With a fused thienothienopyrrolo-thienothienoindole (TTP-TTI) core, BTP-eC9 is a modified version of Y7 but with better solubility. Comparing to Y6, chlorination at the peripheral end-groups can efficiently lower HOMO/LUMO energy levels. C–Cl bond also has a large dipole moment, expanding the absorption range further to near infrared (NIR) region.

High efficient non-flullerene acceptor

High efficient non-fullerene acceptor

With highly conjugated core

Expanded absorption range to near infrared

Expanded absorption range

large dipole moment induced by chloride substituents

Worldwide shipping for BTP-eC9

Worldwide shipping

Quick and reliable shipping

Green energy material

Green energy materials

Processable in non-halogenated solvents

A device efficiency approaching 18% has been reported using BTP-eC9 as the electron acceptor and PBDB-T-2F (PM6) as electron donor in single junction organic photovoltaic cells.

Device structure: ITO/PEDOT:PSS AI 4083/PBDB-T-2F:BTP-eC9 (1:1.2)/PFN-Br/Al

Thickness (nm) VOC (V) JSC (mA cm-2) FF (%) PCE (%)
100 0.839 26.2 81.1 17.8

General Information


CAS Number 2598965-39-8
Chemical Formula C86H94Cl4N8O2S5
Full Name 2,2'- [[12,13-Bis(2-butyloctyl)-12,13-dihydro-3,9-dinonylbisthieno[2'',3'':4',5']thieno[2',3':4,5]pyrrolo[3,2-e:2',3'-g][2,1,3]benzothiadiazole-2,10-diyl]bis[methylidyne(5,6-chloro-3-oxo-1H-indene-2,1(3H)-diylidene) ]]bis[propanedinitrile]
Molecular Weight 1573.89 g/mol
HOMO / LUMO HOMO = -5.64 eV, LUMO = -4.05 eV [1]
Solubility Chloroform, chlorobenzene and dichlorobenzene
Form Dark blue powder/crystal
Synonyms eC9, BTP-eC9, BTPeC9
Classification / Family BTP series NFAs, n-type non-fullerene electron acceptors, Organic semiconducting materials, Low band-gap small molecule, Small molecular acceptor, Organic photovoltaics, Polymer solar cells, NF-PSCs.

Chemical Structure


Chemical structure of BTP-eC9
Chemical structure of BTP-eC9, CAS number: 2598965-39-8

Pricing


Batch Quantity Price
M2249A1 100 mg £330
M2249A1 250 mg £660
M2249A1 500 mg £1190
M2249A1 1 g £1990
M2249A1 5 g / 10 g* Please contact us for details

*for 5 – 10 grams order quantity, the lead time is 4 – 6 weeks.

MSDS Documentation


BTP-eC9 MSDS SheetBTP-eC9 MSDS sheet

Literature and Reviews


  1. Single-Junction Organic Photovoltaic Cells with Approaching 18% Efficiency, Y. Cui et al., Adv. Mater., 32 (19), 1908205 (2020); DOI: 10.1002/adma.201908205.
  2. Self-assembled Monolayer Enables Hole Transport Layer-Free Organic Solar Cells with18% Efficiency and Improved Operational Stability, Y. Lin et al., ACS Energy Lett., 5, 9, 2935–2944 (2020); DOI: 10.1021/acsenergylett.0c01421.
  3. Chlorination: An Effective Strategy for High-Performance. Organic Solar Cells, Q. Zhao et al., Adv. Sci., 7, 2000509 (2020); DOI: 10.1002/advs.202000509.

Related Products


Non-Fullerene Acceptors Collection

Non-Fullerene Acceptors

Non-Fullerene Acceptors

Non-fullerene acceptors (NFAs) are a promising alternative to fullerene-based electron acceptors.

Semiconducting Polymers Collection

Semiconducting Polymers

Semiconducting Polymers

Semiconducting polymers for bulk heterojunction, OPV, OLED, OFET and perovskite interfaces and solar cell research.

Organic Conductors Collection

Organic Conductors

Organic Conductors

Organic conductors are an environmentally friendly alternative to traditional inorganic conductors.

Return to the top