Glass Photoelectrochemical Cells (PECs)

Glass Photoelectrochemical cells for two or three electrode photoelectric effect studies


Our two or three electrode photoelectrochemical cells, designed for photoelectric effect studies, are available with either a glass or polytetrafluoroethylene (PTFE) body. Both types can employ either a two or three-electrode system using a working electrode, a counter electrode and, optionally, a reference electrode.

Photoelectrochemical cells (PECs) are solar cells based on a semiconductor–electrolyte interface. The working electrode, also referred to as photoanode, is normally an n- or p-type semiconductor, i.e. a polymer semiconductor on an ITO/FTO substrate, held by a platinum plate electrode holder. In photoelectrochemical cells, the counter electrode can be platinum or platinum free, i.e. multi-walled carbon nanotubes (MWCNT).

Potentiostat

Ossila Potentiostat
  • Affordable
  • Easy to Use
  • Worldwide Shipping

Buy Online £1550

Specifications

All dimensions are in millimetres.

Glass photoelectrochemical cell specifications
C2017A1: a = 50 mm, b = 55 mm, c = 55 mm.
C2017B1: a = 55 mm, b = 72.5 mm, c = 60 mm.

Pricing and Options

Product Name Product Code Price
Glass Photoelectrochemical Cells - 50 ml C2017A1 £360
Glass Photoelectrochemical Cells - 100 ml C2017B1 £420

To the best of our knowledge the information provided here is accurate. However, Ossila assume no liability for the accuracy of this page. The values provided are typical at the time of manufacture and may vary over time and from batch to batch. All products are for laboratory and research and development use only, and may not be used for any other purpose including health care, military, pharmaceuticals, cosmetics, food, or commercial applications.