Product Code M2349A1-100mg
Price $540

Specifications | MSDS | Literature and Reviews


P5TCN-F25 is a derivative of polythiophenes (PTs) with cyano, fluoro and alkyl groups on the main backbone of the polymer.

The branched 2-hexyldecyl alkyl chains are there to promote the solubility of the polymer and backbone fluorination is believed to lead to stronger interchain interaction, improved polymer crystallinity, and appropriate miscibility with fullerene or non-fullerene acceptors. Meanwhile, the cyano-group on the thiophene ring can not only down-shift the energy levels but also improve the crystallinity of the resulting polymers.

For 5 - 10 grams order quantity please enquire, the lead time is 4-6 weeks.

Luminosyn™ P5TCN-F25


Luminosyn™ P5TCN-F25 is now available.

High purity

P5TCN-F25 is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Batch-specific GPC data

Batch specific GPC data is always available for your thesis or publication

Large-quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


Full name Poly{[3,​3''-​bis(2-​hexyldecyl)​-3'(4')-cyano[2,2':5',2'':5'',2''':5''',2''''-​quinquethiophene]​-​5,​5''''-​diyl]​-alt-[3,​3''-​bis(2-​hexyldecyl)​-3'(4')-cyano-​3''',​4''''-​difluoro[2,2':5',2'':5'',2''':5''',2''''-​quinquethiophene]​-​5,​5''''-​diyl]​}
Synonyms P5TCN-Fx
Chemical formula [(C53H73NS5)0.75(C53H71F2NS5)0.25]n
CAS number n.a.
HOMO / LUMO HOMO = -5.44 eV, LUMO = -3.65 eV [1]
Soluble in Chloroform, chlorobenzene and dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chlorobenzene
Classification / Family Organic semiconducting materials, Low band-gap polymers, Organic Photovoltaics, Polymer solar cells, NF-PSCs.

Batch Details


Batch Mw Mn PDI Stock Info
M2349A1 88,281 39,894 2.21 In stock

Chemical Structure


p5tcn-f25 chemical structure
Chemical structure of P5TCN-F25.

Device Structure


Outstanding device performance with PCE of 17.2% was achieved by using a ternary blend of active layer materials with P5TCN-F25 as the polymer donor and mixed non-fullerene Y6 and fullerene PC71BM as the acceptors by the following device structure.

Device structure: ITO/PEDOT:PSS/P5TCN-F25:Y6:P71CBM/PNDIT-F3N/Ag [1].

Thickness (nm) VOC (V) JSC (mA cm-2) FF (%) PCE (%)
100 0.8 27.55 77.7 17.2

MSDS Documentation


P5TCN-F25 MSDSP5TCN-F25 MSDS sheet

Literature and Reviews


  1. Polythiophenes for organic solar cells with efficiency surpassing 17%,X. Yuan et al., Joule, 6 (3), 647-661 (2022); DOI: 10.1016/j.joule.2022.02.006.
  2. Achieving 16% Efficiency for Polythiophene Organic Solar Cells with a Cyano-Substituted Polythiophene,X. Yuan et al., Adv. Funct. Mater., 2201142 (2022); DOI: 10.1002/adfm.202201142.
Return to the top