It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code B151-1g
Price $648

PCE11 Monomer, used to modify energy gap of polymer semiconducting materials

Free worldwide shipping on qualifying orders


Specifications | MSDS | Literature and Reviews


4-7-bis(5-bromo-4-2-octyldodecylthiophen-2-yl)-5,6-difluorobenzo[c][1,2,5]-thiadiazole, also known as PCE11 monomer (CAS number 1504626-07-6), is a monomer with difluoro attached on benzothiadiazole unit which gives greater electron withdrawn ability to further modify the energy gap of the polymer semiconductor materials. Polymerised with 5,5'-bis(trimethylstannyl)-2,2'-thiophene, PCE11 monomer yields the polymer PffBT4T-2OD (PCE11) which has a power conversion efficiency over 10%.

PCE11 synthesis with 4-7-bis(5-bromo-4-2-octyldodecylthiophen-2-yl)-5,6-difluorobenzo[c][1,2,5]-thiadiazole and 2,5-bis(trimethylstannyl)thieno[3,2-b]thiophene
Synthesis of PCE11 with 4-7-bis(5-bromo-4-2-octyldodecylthiophen-2-yl)-5,6-difluorobenzo[c][1,2,5]-thiadiazole and 2,5-bis(trimethylstannyl)thieno[3,2-b]thiophene
Capped with bromide

Capped with bromide

A PCE11 monomer

Worldwide shipping for 1504626-07-6

Worldwide shipping

Quick and reliable shipping

Fluorinated building block

Benzothiadiazole building block

For semiconductors, OFETs, and solar cells

High purity 1504626-07-6

High purity

>98% High purity

General Information


CAS Number 1504626-07-6
Chemical Formula C54H84Br2F2N2S3
Molecular Weight 1055.26 g/mol
Synonyms PCE11 monomer
PffBT4T-2OD monomer
Classification / Family Benzothiadiazole, Difluorobenzo[c][1,2,5]thiadiazole, Semiconductor synthesis, Low band gap polymers, Acceptors, Organic photovoltaics, Polymer solar cells

Chemical Structure


pce11 monomer
Chemical structure of 4,7-bis(5-bromo-4-(2-octyldodecyl)thiophen-2-yl)-5,6-difluorobenzo[c][1,2,5]thiadiazole, PCE11 monomer

Product Details


Purify >98%
Melting Point N/A
Appearance Red powder

NMR Characterisation


1H NMR pce11-monomer in CDCl3
1H NMR spectrum of 4,7-bis(5-bromo-4-(2-octyldodecyl)thiophen-2-yl)-5,6-difluorobenzo[c][1,2,5]thiadiazole in CDCl3: Instrument AVIIIHD400

MSDS Documentation


PCE11 monomer MSDSPCE11 monomer MSDS sheet

Literature and Reviews


  1. Aggregation and morphology control enables multiple cases of high-efficiency polymer solar cells, Y. Liu, et al., Nat. Comm., 5, 5293 (2014)
  2. Substituent Effects on Physical and Photovoltaic Properties of 5,6-Difluorobenzo[c][1,2,5]thiadiazole-Based D–A Polymers: Toward a Donor Design for High Performance Polymer Solar Cells, Y. Wang, et al., Macromolecules, 46 (24), 9587–9592 (2013).
Return to the top