It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.

ITIC-4F, ITIC-2F, IT-4F

CAS Number 2097998-59-7

Materials, Non-Fullerene Acceptors

Product Code M2075A1-50mg
Price $230

ITIC-4F, high performance acceptor molecule

Non-fullerene acceptor with broad absorption spectrum, 99% purity


Specifications | Pricing and Options | MSDS | Literature and Reviews


Part of our range of non-fullerene acceptors, ITIC-4F (also known as ITIC-2F or IT-4F), CAS number 2097998-59-7, is a derivative of ITIC. Compared to ITIC, ITIC-4F has a better absorption coefficient and a more red-shifted absorption. This can be ascribed to enhanced intramolecular charge transfer. Devices which use ITIC-4F as the electron acceptor can therefore cover a broader absorption spectrum, which may result in a better power conversion efficiency (PCE).

ITIC-4F also has deeper HOMO/LUMO energy levels than ITIC. This makes it a better match for most polymer semiconductor donors, and provides better stability for device fabrication and overall performance. Using an inverted device structure (indium tin oxide (ITO)/ZnO/PBDB-T-SF:TI-4F (1:1)/MoO3/Al [1]), an efficiency of over 13% has been achieved using ITIC-4F as the non-fullerene acceptor and the polymer PBDB-T-SF as the active-layer donor material.

High efficient non-flullerene acceptor

High efficiency non-fullerene acceptor

with highly conjugated core

Better absorption coefficient and red-shifted absorption

Better absorption coefficient and red-shifted absorption

With enhanced intermolecular charge transfer

Worldwide shipping for 1664293-06-4

Worldwide shipping

Quick and reliable shipping

High purity

High purity

>99% High purity

ITIC-F, were it was used

ITIC-4F from Ossila was used in the high-impact paper (IF 18.81), Stretchable and Transparent Conductive PEDOT:PSS-Based Electrodes for Organic Photovoltaics and Strain Sensors Applications, E. Dauzon et al., Adv. Fun. Mater., 30 (28), 2001251 (2020); DOI: 10.1002/adfm.202001251.

Our range of non-fullerene acceptors for highly efficient organic solar cells also includes ITIC and ITIC family members ITIC-DCl, ITIC-M, ITIC-Th, and ITIC-DM. Qualifying orders ship free and all orders are covered by the Ossila Guarantee.

Chemical Structure


Chemical structure of ITIC-4F
Chemical structure of ITIC-4F (ITIC-2F), CAS number: 2097998-59-7

General Information


CAS Number 2097998-59-7
Chemical Formula C94H78F4N4O2S4
Purity 99% (1H NMR)
Full Name 3,9-bis(2-methylene-((3-(1,1-dicyanomethylene)-6,7-difluoro)-indanone))-5,5,11,11-tetrakis(4-hexylphenyl)-dithieno[2,3-d:2’,3’-d’]-s-indaceno[1,2-b:5,6-b’]dithiophene
Molecular Weight 1499.90 g/mol
HOMO / LUMO HOMO = -5.66 eV, LUMO = -4.14 eV [1]
Synonyms ITIC-2F, ITIC-F, IT-4F, ITIC-DF, IT4F
Classification / Family NFAs, organic semiconducting materials, low band-gap small molecule, small molecular acceptor, organic photovoltaics, polymer solar cells, NF-PSCs, n-type acceptor

Pricing


Batch Quantity Price
M2075A1 50 mg £170
M2075A1 100 mg £270
M2075A1 250 mg £540
M2075A1 500 mg £960
M2075A1 1 g £1710

MSDS Documentation


ITIC-2F MSDSITIC-4F (ITIC-2F) MSDS Sheet

Literature and Reviews


  1. Molecular Optimization Enables over 13% Efficiency in Organic Solar Cells, W. Zhao at al., J. Am. Chem. Soc., 139 (21), 7148–7151 (2017); DOI: 10.1021/jacs.7b02677.
  2. Energy-Level Modulation of Small-Molecule Electron Acceptors to Achieve over 12% Efficiency in Polymer Solar Cells, S. Li et al, Adv. Mater., 28, 9423–9429 (2016); DOI: 10.1002/adma.201602776.

Related Products


Non-Fullerene Acceptors Collection

Non-Fullerene Acceptors

Non-Fullerene Acceptors

Non-fullerene acceptors (NFAs) are a promising alternative to fullerene-based electron acceptors.

Semiconducting Polymers Collection

Semiconducting Polymers

Semiconducting Polymers

Semiconducting polymers for bulk heterojunction, OPV, OLED, OFET and perovskite interfaces and solar cell research.

Organic Conductors Collection

Organic Conductors

Organic Conductors

Organic conductors are an environmentally friendly alternative to traditional inorganic conductors.

Return to the top