PTQ10 (CAS number 2270233-86-6) is a donor–acceptor (D–A) type copolymer with a simple thiophene ring as the electron donor unit and quinoxaline (QX) as electron acceptor unit. The alkoxy side chain attached on quinoxaline unit is to promote solubility and to enhance absorption of the targeted polymer. Difluoro substituted quinoxaline can further down-shift the HOMO energy level, achieve fast charge separation and low nonradiative recombination loss in the PSCs leading to high VOC and JSC.

Comparing with some other polymer semiconducting materials, PTQ10 has a simple structure which could lead to mass production with low cost. PTQ10 can also be processed in solution with eco-friendly non-halogenated solvents, i.e. o-xylene. The combined effects of high efficiency, low cost and green solvents processibility makes PTQ10 an ideal candidate for large scale doctor-blading and inkjet printing device fabrications.

Donar-acceptor (D-A) type copolymer

Donor-acceptor (D-A) type copolymer

For high efficient OPV applications

Luminosyn™

Luminosyn™

High purity, batch-specific GPC data, available larger batch orders and higher molecular weight

Worldwide shipping for 2270233-86-6

Worldwide shipping

Quick and reliable shipping

Green energy material

Green energy materials

Processable in non-halogenated solvents

Organic polymer solar cells based on PTQ10:Y6 blend shows efficient charge separation, higher photoluminescence quenching efficiency and higher charge mobilities, giving a power conversion efficiency of 16.53%.

Luminosyn™ PTQ10


Luminosyn™ PTQ10 is now available.

High purity

PTQ10 is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Batch-specific GPC data

Batch specific GPC data is always available for your thesis or publication

Large-quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


Full name Poly [[6,7-difluoro[(2-hexyldecyl)oxy]-5,8-quinoxalinediyl]-2,5-thiophenediyl ]]
Synonyms PTQ10
Chemical formula (C28H36F2N2OS)n
CAS number 2270233-86-6
UV-Vis absorption λmax 556 nm, 600 nm in CB as-cast film
HOMO / LUMO HOMO = -5.54 eV, LUMO = -2.98 eV [1]
Soluble in o-xylene, chloroform, chlorobenzene and dichlorobenzene
Recommended Processing Solvents at 10mg/ml o-xylene (8mg/ml), chloroform
Classification / Family Organic semiconducting materials, Wide band-gap polymers, Organic Photovoltaics, Polymer solar cells, NF-PSCs, All-polymer solar cells (all-pscs), Clean energy materials.

Batch Details


Batch Mw Mn PDI Stock Info
M2283A1 62,379 35,445 1.76 Low stock
M2283A2 74.092 38,464 1.93 In stock

Chemical Structure


PTQ10 chemical structure
Chemical structure of PTQ10

Device Structure


Device structure: ITO (indium tin oxide)/PEDOT:PSS AI 4083/PTQ10:Y6/PDINO/A1 [1]

Thickness (nm) VOC (V) JSC (mA cm-2) FF (%) PCE (%)
110 nm 0.826 26.65 75.1 16.53

MSDS Documentation


PTQ10 MSDSPTQ10 MSDS sheet

Literature and Reviews


  1. Rationally pairing photoactive materials for high-performance polymer solar cells with efficiency of 16.53%, Y. Wu et al., Sci China Chem., 63: 265–271 (2020); DOI: 10.1007/s11426-019-9599-1.
  2. Achieving Fast Charge Separation and Low Nonradiative Recombination Loss by Rational Fluorination for High-Efficiency Polymer Solar Cells, C. Sun et al., Adv. Mater., 31, 1905480 (2019); DOI: 10.1002/adma.201905480.
  3. Exciton and Charge Carrier Dynamics in Highly Crystalline PTQ10:IDIC Organic Solar Cells, H. Cha et al., Adv. Energy Mater., 10 (38) 2001149 (2020); DOI: 10.1002/aenm.202001149.

Return to the top