It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Product Code M2083A4-100mg
Price $594

PCE12, better solubility and film morphology than PCE11

Paired with PC71BM to achieve high device performances


Specifications | Pricing and Options | MSDS | Literature and Reviews


Compared to PffBT4T-2OD (PCE11), PffBT4T-C9C13 has larger side chains which help promote better solubility and film morphology. When using PffBT4T-C9C13 as a polymer donor and PC71BM as electron acceptor (with trimethylbenzene (TMB) as host solvent), a higher device performance of 11.7% was achieved [2].

Due to its broader absorption of the solar spectrum in the visible light region (with an absorption edge at about 800 nm), PffBT4T-C9C13 is also ideal for use as a donor material for all-polymer solar cells and NFA-polymer solar cells

Additionally, its higher solubility means that PffBT4T-C9C13 can be processed with non-halogenated solvents. There are great opportunities with this polymer for inkjet printing on an industrial scale - an environment-friendly approach for alternative renewable energy.

General Information


Full name Poly[(5,6-difluoro-2,1,3-benzothiadiazol-4,7-diyl)-alt-(3,3’’’-di(2-nonyltridecyl)-2,2’;5’,2’’;5’’,2’’’-quaterthiophen-5,5’’’-diyl)]
Synonyms PffBT4T-C9C13, PCE12
Chemical formula (C66H97F2N2S5)n
CAS number n/a
HOMO / LUMO HOMO = -5.34 eV LUMO = -3.69 eV [1]
Solubility/processing solvents Trimethylbenzene (TMB), chlorobenzene
Classification / Family Benzothiadiazole, Fluorinated benzothiadiazole, Heterocyclic five-membered ring, Organic semiconducting materials, Low band gap polymers, Organic photovoltaics, All polymer solar cells, NFA-polymer solar cells

Chemical Structure


hemical structure of PFFBT4T-C9C13 (PCE12)
Chemical structure of PFFBT4T-C9C13 (PCE12)

Pricing


Batch Quantity Price
M2083A1-3 100 mg £440
M2083A1-3 250 mg £1000
M2083A2-3 500 mg £1800
M2083A2-3 1 g £3200
M2083A 5 - 10 g* Please enquire

*For order quantities of 5-10 grams, the lead time is 4-6 weeks.

Batch details


Batch number MW MN PDI Stock Info
M2083A1 123,796 73,818 1.68 Discontinued
M2083A2 136,000 78,000 1.71 Discontinued
M2083A3 118,000 73,000 1.61 Discontinued
M2083A4 143,000 79,000 1.81 In Stock

MSDS Documentation


PCE12 MSDSPCE12 MSDS sheet

Literature and Reviews


  1. Towards a bright future: polymer solar cells with power conversion efficiencies over 10%, Z Hu et al., Sci. China Chem, 60 (5), 571-582 (2017); doi: 10.1007/s11426-016-0424-9.
  2. Efficient organic solar cells processed from hydrocarbon solvents, J. Zhao et al, Nat. Energy 1, 15027 (2016); doi:10.1038/nenergy.2015.27.
Return to the top