DPP-DTT, high quality and high purity semiconducting polymer

High performance p-type polymer and donor material for BHJ photovoltaics


Overview | Specifications | Pricing and Options | MSDS | Literature and Reviews


DPP-DTT is a high mobility p-type polymer, suitable for OFET and sensing and photovoltaic applications.

Ossila's DPP-DTT was used in a high impact paper

DPP-DTT from Ossila was used in the high-impact paper (IF 18.81), Stretchable Mesh-Patterned Organic Semiconducting Thin Films on Creased Elastomeric Substrates, S. Kim et al., Adv. Funct. Mater., 2010870 (2021); DOI: 10.1002/adfm.202010870.

Luminosyn™ DPP-DTT


Luminosyn™ DPP-DTT (also referred to as PDPP2T-TT-OD) is now available.

High molecular weight
Higher molecular weight offers higher charge mobility

High purity
DPP-DTT is purified via Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Batch-specific GPC data
Have confidence in what you are ordering; batch-specific GPC data for your thesis or publications

Large quantity orders
Plan your experiments with confidence with polymers from the same batch

General Information


CAS number 1260685-66-2 (1444870-74-9)
Chemical formula (C60H88N2O2S4)n
HOMO / LUMO HOMO = -5.2 eV, LUMO = -3.5 eV [2]
Synonyms
  • PDBT-co-DTT
  • PTT-DTDPP
  • PDPP-DTT
  • DPPT-TT
  • DPP-TTT
  • PDPP2T-TT
  • PDPP2T-TT-OD
  • DPPDTT
  • Poly[2,5-(2-octyldodecyl)-3,6-diketopyrrolopyrrole-alt-5,5-(2,5-di(thien-2-yl)thieno [3,2-b]thiophene)]
Soluble in o-xylene, chloroform, chlorobenzene and dichlorobenzene
Recommended Processing Solvents o-xylene (8mg/ml), chloroform (10mg/ml)
Classification / Family Bithiophene, Thienothiophene, Organic semiconducting materials, Low band-gap polymers, Organic photovoltaics, Polymer solar cells, OFETs

Chemical Structure


dpp-dtt, PDPP2T-TT-OD, PDBT-co-DTT, 1260685-66-2, 1444870-74-9
Chemical structure and product image of DPP-DTT, CAS 1260685-66-2

Pricing


Batch Quantity Price
M0311A 100 mg £260
M0311A 250 mg £520
M0311A 500 mg £900
M0311A 1 g £1600
M0311A 2 g £2900
M0311A 5 g / 10 g* Please enquire

*For 5 - 10 grams order quantity, the lead time is 4-6 weeks.

Batch Information


Batch Mw Mn PDI Stock info
M0311A10 130,679 46,013 2.84 In Stock

MSDS Documentation


DPP-DTT MSDSDPP-DTT MSDS sheet

OFET and Sensing Applications


The exceptional high mobility of this polymer of up to 10 cm2/Vs [2] via solution-processed techniques, combined with its intrinsic air stability (even during annealing) has made PDPP2T-TT-OD of significant interest for OFET and sensing purposes.

While the highest mobilities require exceptional molecular weights of around 500 kD (and with commensurate solubility issues), high mobilities in the region of 1-3 cm2/Vs can still be achieved with good solution-processing at around 250 kD. As such, we have made a range of molecular weights available to allow for different processing techniques.

In our own tests, we have found that by using simple spin-coating onto an OTS-treated silicon substrate (using our prefabricated test chips), high mobilities comparable to the literature can be achieved (1-3 cm2/Vs). Further improvements may also be possible with more advanced strain-inducing deposition techniques.

DPP-DTT OFET output characteristics DPP-DTT OFET transfer curves DPP-DTT saturation mobility fit DPP-DTT OFET mobility
Example OFET characteristics for DPP-DTT (Batch M311, Mw = 87 kDa, PDI = 4.1) solution processed from chlorobenzene on a 300 nm SiO2 substrate treated with OTS. Output characteristic (top left), transfer curves (top right), mobility fitting (bottom left) and calculated mobility (bottom right).

Photovoltaic Applications


Although shown as a promising hole-mobility polymer for OFETs, when used as the donor material in a bulk heterojunction photovoltaic (with PC70BM as the acceptor), initial efficiencies of 1.6% were achieved for DPP-DTT [3]. The low device metrics were attributed to poor film morphology. However, a higher efficiency of 6.9% was achieved by using thicker film (220 nm) [4].

PDPP2T-TT-OD has also recently been used successfully as an active-layer dopant material in PTB7-based devices [5]. An improvement in device performance was observed, with average efficiencies increasing from 7.6% to 8.3% when the dopant concentration of DPP-DTT was 1 wt%. The use of DPP-DTT as a high-mobility hole-interface layer for perovskite hybrid devices has also been investigated [6].

Synthetic route

DPP-DTT synthesis: DPP-DTT was synthesised by following the procedures described in [2] and [3] (please refer to the following references):

With 2-thiophenecarbonitrile and dimethyl succinate as starting materials in t-amyl alcohol, it gave 3,6-Dithiophen-2-yl-2,5-dihydropyrrolo[3,4-c]pyrrole-1,4-dione. Alkylation of 3,6-Dithiophen-2-yl-2,5-dihydropyrrolo[3,4-c]pyrrole-1,4-dione with 2-octyldodecylbromide in dimethylformamide afforded 3,6-bis(thiophen-2-yl)-2,5-bis(2-octyldodecyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione. Further bromination gave 3,6-bis(5-bromothiophen-2-yl)-2,5-bis(2-octyldodecyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione (M1).

DPP-DTT synthesis procedure to achieve M1

Further reaction of M1 with 2,5-bis(trimethylstannyl)thieno[3,2-b]thiophene (M2) under Stille coupling conditions gave the target polymer DPP-DTT, which was further purified via Soxhlet extraction with methanol, hexane and then chloroform.

DPP-DTT synthesis procedure - reaction of M1 and M2 to achieve DPP-DTT

References


  1. A High Mobility P-Type DPP-Thieno[3,2-b]thiophene Copolymer for Organic Thin-Film Transistors, Y. Li et al., Adv. Mater., 22, 4862-4866 (2010)
  2. A stable solution-processed polymer semiconductor with record high-mobility for printed transistors, J. Li et al., Nature Scientific Reports, 2, 754, DOI: 10.1038/srep00754 (2012)
  3. Synthesis of low bandgap polymer based on 3,6-dithien-2-yl-2,5-dialkylpyrrolo[3,4-c]pyrrole-1,4-dione for photovoltaic applications, G. Zhang et al., Sol. Energ. Mat. Sol. C., 95, 1168-1173 (2011)

Return to the top