It looks like you are using an unsupported browser. You can still place orders by emailing us on info@ossila.com, but you may experience issues browsing our website. Please consider upgrading to a modern browser for better security and an improved browsing experience.


Host material for green PhOLED devices

Exhibits excellent thermal and morphological stability, sublimed ≥99.0%


Specifications | Pricing and Options | MSDS | Literature and Reviews


FATPA, namely 4,4,8,8,12,12-Hexa-p-tolyl-4H-8H-12H-12C-aza-dibenzo[cd,mn]pyrene, is a fully diarylmethylene-bridged triphenylamine (TPA) derivative with six methylphenyl side arms. FATPA has an almost planar triphenylamine core with nitrogen sitting right in the center of carbon and hydrogen structure. With a Tg of 178 °C, FATPA exhibits excellent thermal and morphological stability.

Green phosphorescent OLED device with the novel FATPA as host material and Ir(ppy)3 as triplet emitter shows a maximum current efficiency of 83.5 cd/A and a maximum power efficiency of 71.4 lm/W [1]

General Information


CAS number 1131007-94-7
Chemical formula C63H51N
Molecular weight 822.09 g/mol
Absorption λmax 311 nm (Toluene)
Photoluminescence λem 375 nm (Toluene)
HOMO/LUMO HOMO = 5.22 eV, LUMO = 1.62 eV; ET = 2.78 eV [1]
Chemical name 4,4,8,8,12,12-Hexa-p-tolyl-4H-8H-12H-12C-aza-dibenzo[cd,mn]pyrene
Synonyms 4,4,8,8,12,12-Hexakis(4-methylphenyl)-4H,8H,12H-benzo[1,9]quinolizino[3,4,5,6,7-defg]acridine
Classification / Family Triphenylamine derivatives, Phosphorescent host materials, Sublimed materials, Semiconducting small molecules

Product Details


Purity Sublimed >99.0% (HPLC)
Melting point Tg = 178°C (lit.)
Appearance White powder/crystals

*Sublimation is a technique used to obtain ultra pure-grade chemicals. For more details about sublimation, please refer to the sublimed materials.

Chemical Structure


Chemical structure of FATPA
Chemical structure of FATPA, CAS 1036404-84-8

Device Structure(s)


Device structure ITO/MoO3 (10 nm)/NPB (80 nm)/mCP (5 nm)/FATPA:Ir(ppy)3 (20 nm)/TAZ (40 nm)/LiF (1 nm)/Al (100 nm) [1]
Color green light emitting device Green
Max. Current Efficiency 83.5 cd/A
Max. EQE 23.4%
Max. Power Efficiency 71.4 Im/W

Pricing


Grade Order Code Quantity Price
Sublimed (>99.0% purity) M2290A1 100 mg £220
Sublimed (>99.0% purity) M2290A1 250 mg £440
Sublimed (>99.0% purity) M2290A1 500 mg £760
Sublimed (>99.0% purity) M2290A1 1 g £1300

MSDS Documentation


FATPA MSDSFATPA MSDS sheet

Literature and Reviews


  1. A Fully Diarylmethylene-Bridged Triphenylamine Derivative as Novel Host for Highly Efficient Green Phosphorescent OLEDs, Z. Jiang et al., Org. Lett., 11(7), 1503-6 (2009);DOI:10.1021/ol9001152.
  2. Functionalization of phosphorescent emitters and their host materials by main-group elements for phosphorescent organic light-emitting devices, X. Yang et al., Chem. Soc. Rev., 44, 8484-8575 (2015); DOI: 10.1039/C5CS00424A.
  3. Solution-Processed Undoped Deep-Blue Organic Light-Emitting Diodes Based on Starburst Oligofluorenes with a Planar Triphenylamine Core, C. Liu et al., Chem. Eur. J. 18 (22), 6928-6934 (2012); DOI: 10.1002/chem.201200062.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message