Hydroxyl fullerene, Polyhydroxylated fullerene, Water-soluble C60 fullerene, Fullerenol C60, 99.5% and 99.9% Purity


Fullerenol is a derivative of C60 fullerene with multiple hydroxyl functional groups on its surface. The surface modification of the hydrophobic C60 fullerene with hydroxyl function groups makes fullerene hydrophilic and soluble in polar solvents such as ethanol, DMSO or water. The solubility of fullerenol is dependent on the number of hydroxyl groups attached on the surface of the fullerene ball. Lower degree hydroxylated fullerenols with 10 - 12 hydroxyl groups are soluble in THF, DMF and DMSO, and the medium degree fullerenols with 16 – 24 hydroxyl groups dissolve in more polar solvents such as ethanol and water.

Fullerene acceptor

Fullerene acceptor

Water soluble fullerenes

Multiple functional groups

Versatile applications

Water compatible applications

Worldwide shipping for 115383-22-7

Worldwide shipping

Quick and reliable shipping

High purity

High purity

99.5% and 99.9% Solvent free

Fullerenol has a tendency to aggregate to form nanosized clusters with diameters of 10.7 - 102 nm. The hydroxyl (-OH) groups of the fullerenol is acidic and prone to hydrogen bonding interactions with other fullerenol molecules to form nanoclusters. In aqueous solution, depending on the pH value, fullerenol is more or less deprotonated and exists in the form of stable polyanion nanoparticles.

With great numbers of conjugated double bonds and low residing energy level of lowest unoccupied molecular orbitals (LUMO), fullerenes have been known as radical sponges due to their great ability to scavenge free radicals. For this reason, C60 fullerenol possesses a large radical and cytotoxic activity and it can act as a strong antioxidant.

General Information


CAS Number 182024-42-6
Chemical Formula C60(OH)n
Synonyms Hydroxyl fullerene, Polyhydroxylated fullerene, Water-soluble C60 fullerene, Fullerenol C60
Classification or Family Fullerenes, Electron acceptors, Antioxidants

Product Details


Purity

99.5% (n = 30-50, C60 precursor >99.5%)

99.9% (Solvent free) (n= 30-50, C60 precursor >99.9%)

Solubility > 100 mg/ml in H2O (pH = 7, 25 °C),
Appearance Yellow to light brown powder

Chemical Structure


c60 fullerenol chemical structure
C60 Fullerenol chemical structure

MSDS Documentation


c60 fullerenolC60 Fullerenol MSDS Sheet

Learn More


fullerene c60 Water-Soluble Fullerenes: Preparation and Applications

Water-soluble fullerenes, such as fullerenol C60, are either chemically modified, polymer grafted, or encapsulated in a hydrophillic agent. Fullerenes can then disperse or solubilize in aqueous media. Typical examples of water-soluble fullerenes are polyhydroxylated fullerenes, also knowns as fullerenols, polycarboxylated fullerenes and polysulfonated fullerenes.

Read more...

References


  • A. Djordjevic et al. (2015); Review of Synthesis and Antioxidant Potential of Fullerenol Nanoparticles, J. Nanomater., 567073; DOI: 0.1155/2015/567073.
  • S. Acquah et al. (2017); Review—The Beautiful Molecule: 30 Years of C60 and Its Derivatives, ECS J. Solid State Sci. Technol., 6, M3155; DOI 10.1149/2.0271706jss.
  • J. Grebowski et al. (2013); Fullerenols as a New Therapeutic Approach in Nanomedicine, BioMed Res. Interl., 751913; DOI: 10.1155/2013/751913.

Technical Support


Contact Ossila

To find out more, complete the form below to contact our technical team directly. You can also email info@ossila.com to request a quote or place an order.

Please fill the field
Please enter valid email address
Please enter your message