PBDB-T-2F (CAS number 1802013-83-7) is a PBDB-T family member and, like others, has a high OPV device performance. Polymer solar cells with PBDB-T-2F as the donor and ITIC-2F as the acceptor have achieved a power conversion efficiency (PCE) of over 13%.

By introducing two fluorine atoms to each thiophene unit of the benzodithiophene (BDT) side chains in PBDB-T, the HOMO/LUMO energy levels are pulled. Complete phase separation is observed in the PBDB-T-2F:ITIC-2F blend due to the distinct surface tension difference between PBDB-T-2F and ITIC-2F, resulting in a high domain purity in the blend.

A certified efficiency of 14.9% has been demonstrated using PBDB-T-2F (PM6) as the electron donor and Y6 as an acceptor in a single junction non-fullerene polymer solar cell (NF-PSC) [2].

Conjugated semiconducting polymer

Conjugated semiconducting polymer

As electron donor for high efficient OPV applications

Luminosyn™

Luminosyn™

High purity, batch-specific GPC data, available larger batch orders and higher molecular weight

Worldwide shipping for 1802013-83-7

Worldwide shipping

Quick and reliable shipping

Green energy material

Green energy materials

Processable in non-halogenated solvents

Ossila's PBDB-T-2F used in a high-impact paper

PBDB-T-2F from Ossila was used in the high-impact paper (IF 18.81), Stretchable and Transparent Conductive PEDOT:PSS-Based Electrodes for Organic Photovoltaics and Strain Sensors Applications, E. Dauzon et al., Adv. Fun. Mater., 30 (28), 2001251 (2020); DOI: 10.1002/adfm.202001251; and paper (IF 29.37), Design Rules for Polymer Blends with High Thermoelectric Performance, O. Zapata-Arteaga et al., Adv. Energy Mater., 12, 2104076 (2022); DOI: 10.1002/aenm.202104076.

Luminosyn™ PBDB-T-2F


Luminosyn™ PBDB-T-2F is now available.

High Purity

Purified by Soxhlet extraction with methanol, hexane, and chlorobenzene under an argon atmosphere

Batch-Specific GPC data

Precise molecular weights are always available to provide a reliable reference in your thesis or publication

Large Quantity Orders

Plan and conduct your experiments
with confidence using polymers from the same batch

General Information


Full name Poly[(2,6-(4,8-bis(5-(2-ethylhexyl)-4-fluorothiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene))-alt-(5,5-(1’,3’-di-2-thienyl-5’,7’-bis(2-ethylhexyl)benzo[1’,2’-c:4’,5’-c’]dithiophene-4,8-dione))]
Synonyms PBDB-T-F, PBDB-TF, PM6
Chemical formula (C68H76F2O2S8)n
CAS number 1802013-83-7
HOMO / LUMO HOMO = -5.45 eV, LUMO = -3.65 eV [1]
Processing solvents o-xylene, chloroform, chlorobenzene and dichlorobenzene
Classification / Family Organic semiconducting materials, Medium bandgap polymers, Organic photovoltaics, Polymer solar cells, Perovskite solar cells, Hole-transport layer materials, NF-PSCs, All-polymer solar cells (all-PSCs).

Technical Data


Product Code Soluble in Recommended Processing Solvents at 10mg/ml
M2150A4

Chloroform, chlorobenzene and dichlorobenzene

Chlorobenzene
M2150A5

Chlorobenzene and dichlorobenzene

Dichlorobenzene
M2150A7 Chloroform, chlorobenzene and dichlorobenzene

Dichlorobenzene or Chlorobenzene : dichlorobenzene (v/v = 1:1)

M2150A8/9/10/14

o-Xylene, chloroform, chlorobenzene and dichlorobenzene

o-Xylene (8 mg/ml), chloroform, chlorobenzene
M2150A11/12/13

Chloroform, chlorobenzene and dichlorobenzene

Chloroform, chlorobenzene

Batch Details


Batch Mw Mn PDI Stock info
M2150A13 106,015 44,685 2.37 In stock

Chemical Structure


pbdb-t-2f, pbdb-t-f chemical structure
Chemical structure of PBDB-T-2F, CAS No. 2239295-71-5

MSDS Documentation


PBDB-T-2F MSDSPBDB-T-2F MSDS sheet

Literature and Reviews


  1. Over 14% Efficiency in Organic Solar Cells Enabled by Chlorinated Nonfullerene Small-Molecule Acceptors, H. zhang et al., Adv.Mater., 30, 1800613 (2018); DOI: 10.1002/adma.201800613.
  2. Single-Junction Organic Solar Cell with over 15% Efficiency Using Fused-Ring Acceptor with Electron-Deficient Core, J. Yuan et al., Joule (2019); doi: 10.1016/j.joule.2019.01.004.
  3. Over 14% Efficiency in Polymer Solar Cells Enabled by a Chlorinated Polymer Donor, S. Zhang et al., Adv. Mater., 30, 1800868 (2018); DOI: 10.1002/adma.201800868.

Return to the top