ITO Glass Substrates, 25 mm Square, PV and OLED

Substrates and Fabrication

Product Code S2006C1-100
Price $446

Patterned ITO Substrates for Rapid OLED and PV Prototyping

Large pixels for record breaking-devices


Transmittance | Characterization | Related Products | Resources and Support


The 25 mm square substrates have been designed to help the community take the next step in scaling up active areas. When combined with our deposition masks, these substrates allow four pixels per substrate, with active areas of 48 mm2 each, or a single large pixel with an active area of 255 mm2.

Specifications


Substrate Size 25 mm x 25 mm
Thickness 1.1 mm
Glass Type Polished soda lime, float glass
Substrate Coating Fully oxidized ITO
ITO Thickness 100 nm
ITO Resistance 20 Ω / square
Glass Roughness < 1 nm RMS (By AFM)
ITO Roughness 1.8 nm RMS (By AFM)
Pixel Sizes 48 mm2 (6 mm x 8 mm) or 255 mm2 (15 mm x 17 mm)
ITO 25 x 25 substrate schematic

Transmittance of ITO Substrates

ITO Transmittance

Characterization

AFM scan of ITO substrate
10 µm x 10 µm AFM scan with Z-scale of ±5 nm
AFM of glass surface of ITO substrates
AFM of glass surface (1 µm x 1 µm x 3.5 nm)

Resources and Support


OLED Fabrication GuideOLED Fabrication Guide

Fabricating OLED devices using Ossila’s pre-patterned ITO substrates is designed to be quick and easy. We've included every detail that we can in this manual so that you can produce efficient devices with as little effort as possible.

Read more...
OPV Fabrication GuideOPV Fabrication Guide

Within this guide, you’ll find comprehensive explanations for each step, along with additional tips and insights we’ve gathered to help you achieve the best possible results.

Read more...