PBDB-TF-T1 is a randomly copolymerised conjugated semiconducting polymer with benzodithiophene (BDT), Benzodithiophene dione (BDD) and thiophene carboxylate ester as the main backbone units. PBDB-TF-T1 is a close relative in structure to PBDBT-2F (PM6) and PTO2, relatively blue shifted in absorption to PM6 and red shifted to PTO2.
PBDB-TF-T1 is also relatively more soluble in non-halogenated solvents, i.e. o-xylene, 1,2,4‐trimethylbenzene or THF than PM6. Non-fullerene polymer solar cells withnon-halogenated solvent additive DIO from BTP-4F-12 as acceptor and PBDB-TF-T1 as polymer donor achieved high device performance efficiencies of PCE = 16.1%.
Conjugated semiconducting polymer
For high efficient OPV applications
Luminosyn™
High purity, batch-specific GPC data, available larger batch orders and higher molecular weight
Worldwide shipping
Quick and reliable shipping
Green energy materials
Processable in non-halogenated solvents
Luminosyn™ PBDB-TF-T1
Luminosyn™ PBDB-TF-T1 is now available.
High purity
PBDB-TF-T1 is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere
Batch-specific GPC data
Batch specific GPC data is always available for your thesis or publication
Large-quantity orders
Plan your experiments with confidence with polymers from the same batch
General Information
CAS Number | N/A |
---|---|
Chemical Formula | [(C68H76F2O2S8)0.8(C41H44F2O2S5)0.2]n |
Full Name | Poly[(2,6-(4,8-bis(5-(2-ethylhexyl)-4-fluoro)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene)-alt-(5,5-(1’,3’-di-2-thienyl-5’,7’-bis(2-ethylhexyl)benzo[1’,2’-c:4’,5’-c’]dithiophene-4,8-dione))]-ran-poly[(2,6-(4,8-bis(5-(2-ethylhexyl)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene))-alt-(2,2-ethyl-3(or4)-carboxylate-thiophene)] |
HOMO / LUMO | HOMO = -5.48 eV, LUMO = -3.63 eV [1] |
Soluble in | o-Xylene, chloroform, chlorobenzene and dichlorobenzene |
Recommended Processing Solvents at 10mg/ml | Dichlorobenzene or Chlorobenzene+dichlorobenzene (1:1 v/v) |
Synonyms | T1 |
Classification / Family | Organic semiconducting materials, Medium band-gap polymers, Organic Photovoltaics, Polymer solar cells, NF-PSCs, All-polymer solar cells (all-pscs). |
Batch Details
Batch | Mw | Mn | PDI | Stock Info |
---|---|---|---|---|
M2259A1 | 99,351 | 42,777 | 2.32 | In Stock |
Chemical Structure

Device Structure
Device structure: ITO/PEDOT:PSS AI 4083/T1:BTP-4F-12/PFN-Br/Al. [2]
Thickness (nm) | VOC(V) | JSC(mA cm-2) | FF(%) | PCE(%) |
---|---|---|---|---|
N/A | 0.853 | 25.2 | 76 | 16.1 |
MSDS Documentation
Literature and Reviews
- Achieving Over 15% Efficiency in Organic Photovoltaic Cells via Copolymer Design, Y. Cui et al., Adv. Mater., 31 (14), 1808356 (2019); DOI: 10.1002/adma.201808356.
- Eco-Compatible Solvent-Processed Organic Photovoltaic Cells with Over 16% Efficiency, L Hong et al., Adv. Mater., 31 (39), 1903441 (2019); DOI: 10.1002/adma.201903441..