PBDB-TF-T1, high purity semiconducting polymer

High quality and available for fast, secure dispatch


Specifications | MSDS | Literature and Reviews


PBDB-TF-T1 is a randomly copolymerised conjugated semiconducting polymer with benzodithiophene (BDT), Benzodithiophene dione (BDD) and thiophene carboxylate ester as the main backbone units. PBDB-TF-T1 is a close relative in structure to PBDBT-2F (PM6) and PTO2, relatively blue shifted in absorption to PM6 and red shifted to PTO2.

PBDB-TF-T1 is also relatively more soluble in non-halogenated solvents, i.e. o-xylene, 1,2,4‐trimethylbenzene or THF than PM6. Non-fullerene polymer solar cells withnon-halogenated solvent additive DIO from BTP-4F-12 as acceptor and PBDB-TF-T1 as polymer donor achieved high device performance efficiencies of PCE = 16.1%.

Conjugated semiconducting polymer

Conjugated semiconducting polymer

For high efficient OPV applications

Luminosyn™

Luminosyn™

High purity, batch-specific GPC data, available larger batch orders and higher molecular weight

Worldwide shipping for PBDB-TF-T1

Worldwide shipping

Quick and reliable shipping

Green energy material

Green energy materials

Processable in non-halogenated solvents

Luminosyn™ PBDB-TF-T1


Luminosyn™ PBDB-TF-T1 is now available.

High purity

PBDB-TF-T1 is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Batch-specific GPC data

Batch specific GPC data is always available for your thesis or publication

Large-quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


CAS Number N/A
Chemical Formula [(C68H76F2O2S8)0.8(C41H44F2O2S5)0.2]n
Full Name Poly[(2,6-(4,8-bis(5-(2-ethylhexyl)-4-fluoro)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene)-alt-(5,5-(1’,3’-di-2-thienyl-5’,7’-bis(2-ethylhexyl)benzo[1’,2’-c:4’,5’-c’]dithiophene-4,8-dione))]-ran-poly[(2,6-(4,8-bis(5-(2-ethylhexyl)thiophen-2-yl)-benzo[1,2-b:4,5-b’]dithiophene))-alt-(2,2-ethyl-3(or4)-carboxylate-thiophene)]
HOMO / LUMO HOMO = -5.48 eV, LUMO = -3.63 eV [1]
Soluble in o-Xylene, chloroform, chlorobenzene and dichlorobenzene
Recommended Processing Solvents at 10mg/ml Dichlorobenzene or Chlorobenzene+dichlorobenzene (1:1 v/v)
Synonyms T1
Classification / Family Organic semiconducting materials, Medium band-gap polymers, Organic Photovoltaics, Polymer solar cells, NF-PSCs, All-polymer solar cells (all-pscs).

Batch Details


Batch Mw Mn PDI Stock Info
M2259A1 99,351 42,777 2.32 In Stock

Chemical Structure


pbdb-tf-t1 chemical structure and solubility in o-xylene
Chemical structure of PBDB-TF-T1 (T1) and its solubility in o-xylene

Device Structure


Device structure: ITO/PEDOT:PSS AI 4083/T1:BTP-4F-12/PFN-Br/Al. [2]

Thickness (nm) VOC(V) JSC(mA cm-2) FF(%) PCE(%)
N/A 0.853 25.2 76 16.1

MSDS Documentation


PBDB-TF-T1 MSDSPBDB-TF-T1 MSDS Sheet

Literature and Reviews


  1. Achieving Over 15% Efficiency in Organic Photovoltaic Cells via Copolymer Design, Y. Cui et al., Adv. Mater., 31 (14), 1808356 (2019); DOI: 10.1002/adma.201808356.
  2. Eco-Compatible Solvent-Processed Organic Photovoltaic Cells with Over 16% Efficiency, L Hong et al., Adv. Mater., 31 (39), 1903441 (2019); DOI: 10.1002/adma.201903441..