PCE8, electron acceptor in highly-efficient all-PSCs

High quality polymer available with free shipping on qualifying orders


Specifications | MSDS | Literature and Reviews


PNDI(2OD)T (also known as PCE8), CAS number 1236111-76-4, is a family member of polynaphthalene diimide. It has successfully been used as an electron acceptor in highly-efficient all-polymer solar cells (all-PSCs), achieving a record performance with PCE of 8% [1].

Compared to PC71BM, PNDI(2OD)T has lower-lying HOMO and higher-lying LUMO energy levels, which could potentially lead to higher open voltages in all-PSC devices.

PNDI(2OD)T also exhibits n-channel characteristics in organic field-effect transistor (OFET) devices, with its electron mobility (μe,FET) value being up to 0.25 cm2V−1 s-1 [2].

Luminosyn™ PNDI(2OD)T


Luminosyn™ PNDI(2OD)T is now available.

High molecular weight and high purity

PNDI(2OD)T is purified by Soxhlet extraction with methanol, hexane and chlorobenzene under an argon atmosphere

Large quantity orders

Plan your experiments with confidence with polymers from the same batch

General Information


Full name Poly[[1,​2,​3,​6,​7,​8-​hexahydro-​2,​7-​bis(2-​octyldodecyl)​-​1,​3,​6,​8-​tetraoxobenzo[lmn]​[3,​8]​phenanthroline-​4,​9-​diyl]​-​2,​5-​thiophenediyl]
Synonyms
  • PCE8
  • PNDI-T
  • P(NDI2OD-T)
  • Poly{[N,N'-bis(2-octyldodecyl)naphthalene-1,4,5,8-bis(dicarboximide)-2,6-diyl]-alt-2,5-thiophene}
Chemical formula (C58H86N2O4S)n
CAS number 1236111-76-4
HOMO / LUMO HOMO = -6.52 eV, LUMO = -4.04 eV [1]
Classification / Family PNDI polymers, Organic n-type semiconducting materials, PNDI polymers, Organic photovoltaics, All-Polymer solar cells (all-PSCs), Electron-acceptor polymers, OFETs, Perovskite solar cells.
Soluble in Chloroform, chlorobenzene, dichlorobenzene
Recommended Processing Solvents at 10mg/ml Chloroform

Batch Details


Batch number MW Mn PDI Stock info
M2087A1 77,791 174,105 2.23 Low stock
M2087A2 25,298 43,113 1.70 In stock

Chemical Structure


Chemical structure of PNDI(2OD)T (PCE8)
Chemical structure of PNDI(2OD)T (PCE8)

MSDS Documentation


PNDI(2OD)T MSDSPNDI(2OD)T MSDS sheet

Literature and Reviews


  1. 8.0% Efficient All-Polymer Solar Cells with High Photovoltage of 1.1 V and Internal Quantum Efficiency near Unity, X Xu et al.,, Adv. Energy Mater., 8, 1700908 (2018); DOI: 10.1002/aenm.201700908.
  2. Importance of Electron Transport Ability in Naphthalene Diimide-Based Polymer Acceptors for High-Performance, Additive-Free, All-Polymer Solar Cells, J. Choi et al., Chem. Mater., 27 (15), 5230–5237 (2015); DOI: 10.1021/acs.chemmater.5b01274.